首页> 外文期刊>Refractories and Industrial Ceramics >Resistance of Refractories of the Al2O3-Cr2O3 System Under Liquid-Phase Reduction Conditions of Iron-Containing Technogenic Waste
【24h】

Resistance of Refractories of the Al2O3-Cr2O3 System Under Liquid-Phase Reduction Conditions of Iron-Containing Technogenic Waste

机译:Al2O3-CR2O3系统耐耐药性耐液相减少条件下耐铁技术废弃物的抗性

获取原文
获取原文并翻译 | 示例
           

摘要

Results are provided for a laboratory study of the applicability of refractories in the Al2O3-Cr2O3 system in bubble-agitated double-chamber laboratory furnaces during processing of a broad spectrum of iron-containing materials, including technogenic waste. Laboratory tests are conducted for refractory life in a medium of molten iron. Conditions are modeled for exploitation of a refractory in melting and reducing zones of a bubble-agitated type furnace. Optical microscopy is used to study zones and the overall depth of crucible reaction with melt at the melt - refractory crucible interface.
机译:在加工型含铁材料的加工过程中,提供了在燃气搅拌双室实验室炉中Al2O3-CR2O3系统中耐火材料的适用性的实验室研究。 在铁水介质中进行实验室测试以进行耐火寿命。 用于利用熔化和减少气泡型炉子的熔化区的耐火材料的调节条件。 光学显微镜用于研究区和熔融 - 耐火坩埚界面的熔体的坩埚反应的整体深度。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号