Influence of flexible spacer length on self-organization behaviors and photophysical properties of hemiphasmidic liquid crystalline polymers containing cyanostilbene

机译:柔性间隔率对含有CyanostiLbene的自组织行为对自组织行为的影响及赤骨液晶聚合物的光物理性能

获取原文
获取原文并翻译 | 示例
           

摘要

A series of hemiphasmidic luminescent liquid crystalline polymers, in which the hemiphasmidic mesogen containing cyanostilbene were linked to the polymethacrylate main-chains via flexible spacers with different lengths, named poly {(Z)-m-(4-(1-cyano-2-(3,4,5-tris(octyloxy)phenyl)vinyl)phenoxy)alkyl methacrylatel (donated as Pr-m, m = 2, 4, 6, 8, 10) were synthesized via free radical polymerization. The phase structures and photophysical properties of Pr-m were investigated in detail by a combination of techniques including differential scanning calorimetry (DSC), polarizing optical microscopy (POM), small-angle X-ray scattering (SAXS), UV-Vis absorption spectra (UV-Vis spectra), photoluminescence spectra (PL spectra) and particle size analyzer. The results revealed that the phase structures of Pr-m transformed from hexagonal columnar phase (m = 2, 4) to smectic A phase (m = 6, 8, 10) with the increasing of flexible spacer length. All of the polymers featured similar AIEE properties, however, the solid state quantum yields of Pr-m decreased with the increasing flexible spacer length, and the solid quantum yields of Pr-m decreased from 8.55 (Pr-2) to 3.71 (Pr-10) with the increasing flexible spacer length.
机译:一系列偏瘫发光液晶聚合物,其中含六氨脱色的氰蛋白酶通过具有不同长度的柔性间隔物与聚甲基丙烯酸酯的主链连接,具有不同的长度,命名为poly {(z)-m-(4-(1-氰基-2- (3,4,5- Tris(辛氧基)苯基)乙烯基)苯氧基)通过自由基聚合合成烷基甲基丙烯酸烷基甲基丙烯酰基甲基丙烯酸烷基甲基丙烯酰基(捐赠为PR-M,M = 2,4,6,8,10)。通过包括差示扫描量热法(DSC),偏振光学显微镜(POM),小角X射线散射(SAX),UV-Vis吸收光谱的技术的组合详细研究了PR-M的相结构和光学性质。 (UV-VIS光谱),光致发光光谱(PL光谱)和粒度分析仪。结果表明,PR-M的相结构从六方柱状相(M = 2,4)转化为次相(m = 6,8,10)的柔性间隔物长度的次相(m = 6,8,10)。所有聚合物都具有类似的AIEE特性,然而,PR-M的固态量子产率随着柔性间隔长度的增加而降低,PR-M的固量产率从8.55(PR-2)降至3.71(PR- 10)随着柔性的间隔长度的增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号