In the present work, fracture resistance of two types of hot mix asphalt (HMA) mixtures (i.e. the first one contained a normal binder, and the second one contained the same binder but modified by crumb rubber of recycled tyres) was successfully characterized using an asymmetric disc bend specimens. The experiments were performed under different loadings of pure mode I, pure mode II and two mixed mode I/III at three subzero temperatures. The HMA mixture contained crumb rubber was found to more resist against the fracture than that contained the normal binder. The results also showed that by decreasing the temperature, fracture resistance of the HMA mixtures first increased and then reduced. In addition, as the proportion of mode III at the crack tip (from pure mode I to pure mode III) increased, the HMA resistance against the crack growth reduced. Meanwhile, for the pure mode I loading, the crack growth path was along the initial crack; while, by adding the mode III to the mode I at the crack tip, the crack growth path twisted correspondingly further. (C) 2017 Elsevier Ltd. All rights reserved.
机译:在本作本作中,两种类型的热混合沥青(HMA)混合物的断裂抗性(即第一个含有正常粘合剂,第二个含有相同的粘合剂但由再循环轮胎的碎屑橡胶改性)进行了一种不对称盘弯曲标本。在三个子单温度下在纯模式I,纯模式II和两个混合模式I / III的不同载荷下进行实验。含有碎屑橡胶的HMA混合物比含有正常粘合剂的抗骨折更抗蚀剂。结果还表明,通过降低温度,HMA混合物的断裂抗性首先增加,然后减少。另外,作为裂纹尖端(从纯模式I到纯模式III)的模式III的比例增加,HMA抗裂纹增长的抗性降低。同时,对于纯模式I加载,裂缝的增长路径沿着初始裂缝;虽然,通过将模式III添加到裂缝尖端的模式I,而裂缝的增长路径相应地进一步扭曲。 (c)2017 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号