This work was aimed to produce elongated nanoparticles of clinical interest by the stretching method. Polymer films prepared from material recovered from the dissolution of a marketed stretchable water-soluble film were loaded with 10% of poly(isobutylcyanoacrylate) nanoparticles. The films were elongated at 50 degrees C to 230% of their initial lengths. The shape factor of the nanoparticles recovered after elongation was consistent with stretching conditions applied on the film. This work has demonstrated the feasibility of the preparation of nonspherical poly(isobutylcyanoacrylate) nanoparticles by the stretching method and described conditions to apply the method.
机译:这项工作旨在通过拉伸方法生产临床兴趣的细长纳米粒子。 由从销售可拉伸水溶性薄膜溶解的材料中回收的材料制备的聚合物膜,其10%的聚(异丁基丙烯酸盐)纳米颗粒。 将薄膜以50℃伸长至初始长度的230%。 在伸长率后回收的纳米颗粒的形状因子与施加在薄膜上的拉伸条件一致。 该工作表明,通过拉伸方法制备非球形聚(异丁基丙烯酸酯)纳米颗粒的可行性,并描述了应用该方法的条件。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号