Effect of surface contamination on the durability and strength of stainless steel - polyisobutylene pressure-sensitive adhesive bonds

机译:表面污染对不锈钢 - 聚异丁烯压敏粘合剂耐久性和强度的影响

获取原文
获取原文并翻译 | 示例
           

摘要

Cleaning of substrates surface with a solvent is a standard step in a procedure of adhesive joints preparation while carrying out adhesion tests. However, is cleanliness of substrates really so important? The effect of contamination of substrates surfaces with vegetable (sunflower) and mineral (naphthenic) oils on the strength and durability of adhesive joints formed by neat and organoclay-filled polyisobutylene-based PSAs with a stainless steel substrate was studied. For the filled composition, the strength of the adhesive joints was higher, even with the contaminated surface, than for the system with the neat PIB. Contamination of the surface leads to the formation of a weak layer of plasticized polymer, which contributes to decreasing of the adhesion strength and durability. These parameters, however, are restored over time, which could be connected with the absorption of the contaminants by the adhesive material, as a result of polymer swelling, and their migration to the bulk of the adhesive. The ability of contaminants that can be absorbed and removed from the surface into the bulk of the adhesive is determined by their solubility in the adhesive. It was demonstrated using laser microinterferometry method that PIB is miscible with naphthenic oil, whereas PIB - sunflower oil system exhibits upper-criticalsolution-temperature behavior. These observations provide an explanation to the growth trends of durability and strength of the joints over time in the cases of sunflower and naphthenic oil contamination of the substrate's surface.
机译:用溶剂清洁基板表面是粘合接头制备的过程中的标准步骤,同时进行粘附试验。但是,基材的清洁度真的如此重要吗?研究了用蔬菜(向日葵)和矿物(环烷)和矿物(环烷基)油对由纯净的基于粘合剂的粘合剂的强度和耐久性与不锈钢基板形成的粘合剂的强度和耐久性的影响。对于填充的组合物,粘合剂接头的强度甚至含有污染的表面,而不是用纯PIB的系统。表面的污染导致形成粘合聚合物的弱层,这有助于降低粘合强度和耐久性。然而,这些参数随时间恢复,其可以通过粘合材料的污染物的吸收而与聚合物溶胀的结果相连,并将其迁移到大量粘合剂的偏移。通过其在粘合剂中的溶解度确定可以从表面吸收和除去的污染物的能力。使用激光微吸入法证明PIB与环烷体混溶的方法,而PIB - 葵花籽油系统表现出上部 - 临界温度行为。这些观察结果对底物表面的向日葵和环烷油污染的情况下,对关节的耐用性和强度的增长趋势提供了解释。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号