摘要

Magnesium oxide (MgO) with different morphology were prepared by calcining precursors (magnesium hydroxide MH). The precursors were synthesized from industry lightly calcined powder (MgO content of 80-93%) by ammonia circulation method. The structures of MH and MgO were characterized by scanning electron microscope and laser particle size analyzer. The crystal growth mechanism of MgO precursors were simulated by materials studio. The experimental results showed that the MgO had the same morphology with their precursors. The adsorption of SO42 can significantly increase the particle size of precursors, and its D-50 reached 2.05 mu m. After adsorping Cl-, the exposure proportion of planes (001) and (101) was reduced, and the morphology of MH more easily grow to be uniform bulk crystal. The activity of MgO (CAA) produced with MgCl2 was 150085 by the citric acid method, which was higher than other MgO produced with Mg(NO3)(2) and MgSO4. (C) 2016 Published by Elsevier B. V. on behalf of The Society of Powder Technology Japan. All rights reserved.
机译:通过煅烧前体(氢氧化镁MH)来制备具有不同形态的氧化镁(MgO)。通过氨循环法从工业轻度煅烧粉末(MgO含量为80-93%)合成前体。 MH和MgO的结构通过扫描电子显微镜和激光粒度分析仪表征。材料工作室模拟了MgO前驱体的晶体生长机理。实验结果表明,MgO的形态与它们的前体相同。 SO42的吸附可显着增加前驱体的粒径,其D-50达到2.05μm。吸附Cl-后,平面(001)和(101)的暴露比例降低,MH的形态更容易生长为均匀的块状晶体。柠檬酸法用MgCl2生成的MgO(CAA)的活性为150085,高于用Mg(NO3)(2)和MgSO4生成的其他MgO的活性。 (C)2016由Elsevier B.V.代表日本粉末技术学会出版。版权所有。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号