Corrosion behavior of X80 pipeline steel in the presence of Brevibacterium halotolerans in Beijing soil

机译:X80管线钢在北京土壤中霍曲杆菌的存在下的腐蚀行为

获取原文
获取原文并翻译 | 示例
           

摘要

In this study, the corrosion behavior of X80 pipeline steel in the presence of Brevibacterium halotolerans (B. halotolerans) was investigated by surface analysis and electrochemical measurements. Results show that B. halotolerans can attach to the surface of X80 steel, and the entire surface is covered with B. halotolerans. The corrosion products induced by B. halotolerans were FeOOH, Fe2O3 and FeSO4. X80 steel corrosion was accelerated in the presence of B. halotolerans and was susceptible to pitting corrosion. The formation of pitting corrosion could be due that the B. halotolerans oxidization of elemental iron in X80 steel to either obtain electrons from the reduction of nitrate in the underlying biofilm or in the damaged corrosion product film. (C) 2018 Elsevier B.V. All rights reserved.
机译:在这项研究中,通过表面分析和电化学测量研究了X80管线钢在短边钾(B.Halotolerans)存在下的腐蚀行为。 结果表明,B. NaLotolerans可以连接到X80钢的表面,并且整个表面被B. Halotolans覆盖。 B.Halotolerans诱导的腐蚀产品是FeOOH,Fe2O3和FesO4。 X80 X80钢腐蚀在B. NaLotolerans存在下加速,并且易于蚀腐蚀。 蚀腐蚀的形成可能是由于B.Alotolerans在X80钢中的元素铁氧化,以获得来自下面的生物膜中的硝酸盐的还原物或受损的腐蚀产物膜。 (c)2018 Elsevier B.v.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号