Deterioration of residential concrete foundations: The role of pyrrhotite-bearing aggregate

机译:住宅混凝土基金会的恶化:铅球菌骨料骨料的作用

获取原文
获取原文并翻译 | 示例
           

摘要

Premature deterioration of concrete foundations has been reported for a large number of homes in Eastern Connecticut of the United States. The characteristic symptoms are map cracking, whitish deposits at the vicinity of the cracking surface and wide crack opening. It is hypothesized that the volume expansion associated with the oxidation of pyrrhotite-bearing aggregate and the following internal sulfate attack (ISA) due to the delayed secondary mineral formation are the primary causes of premature deterioration. Extensive tests were carried out to validate the hypothesis using a combination of tools such as scanning electron microscopy (SEM), X-ray diffraction (XRD), X-ray fluorescence (XRF) and energy dispersive X-ray (EDX).
机译:据报道,美国东部康涅狄格州的大量房屋据报道了混凝土基金会的过早恶化。 特征症状是地图开裂,白色沉积物在裂缝表面附近和宽裂纹开口。 假设由于延迟的二级矿物质形成导致的含有烟道石骨料的氧化和下列内硫酸盐发作(ISA)相关的体积膨胀是过早劣化的主要原因。 进行广泛的测试以使用诸如扫描电子显微镜(SEM),X射线衍射(XRD),X射线荧光(XRF)和能量分散X射线(EDX)的工具的组合来验证假设。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号