The aim of this study was to employ an experimental protocol for in vivo evaluation of sols of 5 wt.% poly(ethylene glycol) (PEG) in phosphate-buffered saline as artificial vitreous substitutes. A 20 gauge pars plana vitrectomy and posterior vitreous detachment were performed in the right eye of eight pigmented rabbits. Approximately 1 ml of the viscoelastic PEG sols was then injected into the vitreous space of six eyes. PEG with an average molecular weight of 300,000 and 400,000 g mol(-1) was used in two and four eyes, respectively. Two eyes received balanced salt solution and served as controls. Full-field electroretinography was carried out and intra-ocular pressure (IOP, palpation) measured pre- and post-operatively at regular intervals up to 41 days. The rabbits were killed and the eyes examined by retinal photography, gross macroscopic examination and histology. The viscoelastic sols were successfully injected and remained translucent throughout the post-operative period, with some inferior formation of precipitates. None of the eyes displayed IOP elevation post-operatively, but in three of the PEG sol injected eyes transient hypotony was noted. One eye sustained retinal detachment during surgery and another two in the post-operative period. ERG recordings confirmed preservation of retinal function in three out of four eyes injected with 400,000 g mol(-1) PEG. Histological examination revealed up-regulation of glial acidic fibrillary protein in Muller cells in PEG sol injected eyes, but normal overall morphology in eyes with attached retinas. The viscosity of the sol was not retained throughout the post-operative period, indicating the demand for polymer cross-linking to increase residence time. The results provide promising preliminary results on the use of PEG hydrogels as a vitreous substitute.
机译:这项研究的目的是采用一种实验方案,对磷酸盐缓冲液中5 wt。%聚乙二醇(PEG)溶胶作为人工玻璃体替代物进行体内评估。在八只有色兔子的右眼中进行了20号尺的玻璃体平面切除术和玻璃体后脱离。然后将约1ml的粘弹性PEG溶胶注入六只眼的玻璃体腔中。分别在两只和四只眼中使用平均分子量分别为300,000和400,000 g mol(-1)的PEG。两只眼睛接受平衡的盐溶液并作为对照。进行全视野视网膜电图检查,并在术前和术后定期测量眼内压(IOP,触诊),直至41天。杀死兔子并通过视网膜摄影,肉眼宏观检查和组织学检查眼睛。粘弹性溶胶已成功注入,并在整个术后期间保持半透明状态,形成的沉淀物较差。术后没有一只眼睛显示出眼压升高,但是在三只PEG溶胶注射的眼睛中发现了短暂的低渗。一只眼睛在手术过程中持续视网膜脱离,另一只眼睛在术后阶段。 ERG记录证实注射了400,000 g mol(-1)PEG的四只眼睛中有三只保留了视网膜功能。组织学检查显示,注射PEG溶胶的眼睛中Muller细胞中的胶质酸性纤维蛋白上调,但附有视网膜的眼睛的总体形态正常。溶胶的粘度在整个术后期间没有保留,表明需要聚合物交联以增加停留时间。该结果提供了关于使用PEG水凝胶作为玻璃体替代物的有希望的初步结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号