The characteristics of adhesive properties between a denture base and resilient denture liner were investigated by a modified peel test with an L-shaped metal attachment. Three commercially resilient denture lining materials, namely GC Reline Soft (S), GC Reline Extra Soft (ES), and GC Reline Ultra Soft (US), were evaluated. Acrylic resin (GC Acron) was used as denture base material. Peel specimens consisting of the denture base acrylic resin and resilient denture liner were tested after storage for 1 and 30 days in distilled water at 37 degrees C. The modified peel test method gave load-displacement curves and work of adhesion (W(A)) values of the denture base material and resilient denture liner. The W(A) of specimens after 1 day of storage ranged from 1.71 to 2.55 N mm(-1) and increased in the order from US to S to ES. On the other hand, the W(A) of specimens after 30 day of storage ranged from 1.44 to 2.47 N mm(-1) and increased in the order from US to ES to S. US had significantly lower W(A) after 1 and 30 days of storage than did S and ES (P<0.05). Comparison of the W(A) between 1 and 30 days, reveals large differences for ES and US, but not for S. This could be explained by the difference in failure modes. Within the limitations of this investigation, it was concluded the modified peel test is effective for evaluating the adhesion between denture base material and a resilient denture liner.
机译:通过带有L形金属附件的改良剥离试验研究了义齿基托和弹性义齿衬里之间的粘合特性。评估了三种具有商业弹性的义齿衬里材料,即GC Reline Soft(S),GC Reline Extra Soft(ES)和GC Reline Ultra Soft(US)。丙烯酸树脂(GC Acron)用作义齿基材。在37°C的蒸馏水中储存1天和30天后,对由义齿基体丙烯酸树脂和弹性义齿衬里组成的剥离样品进行了测试。改良的剥离试验方法给出了载荷-位移曲线和粘附功(W(A))义齿基体材料和弹性义齿衬里的数值。储存1天后,样品的W(A)从1.71到2.55 N mm(-1),并且从US到S到ES依次增加。另一方面,样品在储存30天后的W(A)从1.44到2.47 N mm(-1)不等,并且从US到ES到S依次增加。US在1天后的W(A)显着降低。和储存30天比S和ES​​(P <0.05)。比较1天和30天之间的W(A),发现ES和US的差异很大,而S的差异不大。这可以用故障模式的差异来解释。在这项研究的范围内,可以得出结论,改进的剥离测试对于评估义齿基体材料和弹性义齿衬里之间的附着力是有效的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号