For selective leaching and highly effective recovery of heavy metals from a metallurgical sludge, a two-step leaching method was designed based on the distribution analysis of the chemical fractions of the loaded heavy metal. Hydrochloric acid (HCl) was used as a leaching agent in the first step to leach the relatively labile heavy metals and then ethylenediamine tetraacetic acid (EDTA) was applied to leach the residual metals according to their different fractional distribution. Using the two-step leaching method, 82.89% of Cd, 55.73% of Zn, 10.85% of Cu, and 0.25% of Pb were leached in the first step by 0.7 M HCl at a contact time of 240 min, and the leaching efficiencies for Cd, Zn, Cu, and Pb were elevated up to 99.76, 91.41, 71.85, and 94.06%, by subsequent treatment with 0.2 M EDTA at 480 min, respectively. Furthermore, HCl leaching induced fractional redistribution, which might increase the mobility of the remaining metals and then facilitate the following metal removal by EDTA. The facilitation was further confirmed by the comparison to the one-step leaching method with single HCl or single EDTA, respectively. These results suggested that the designed two-step leaching method by HCl and EDTA could be used for selective leaching and effective recovery of heavy metals from the metallurgical sludge or heavy metal-contaminated solid media.
机译:对于从冶金污泥的选择性浸出和高效恢复重金属,基于装载重金属化学级分的分布分析设计了一种两步的浸出方法。在第一步中使用盐酸(HCl)作为浸出的浸出剂,以浸入相对不稳定的重金属,然后根据其不同的分布分布施用乙二胺四乙酸(EDTA)以浸入残留金属。使用两步浸出方法,82.89%的Cd,55.73%的Zn,10.85%Cu,以及0.25%的Pb在第一步中在240分钟的接触时间和浸出效率下浸出0.7μmHCl对于Cd,Zn,Cu和Pb,通过随后在480分钟的情况下进行0.2M EDTA的治疗,Zn,Cu和Pb高达99.76,91.41,71.85和94.06%。此外,HCl浸出诱导的分数重新分布,这可能增加剩余金属的迁移率,然后促进EDTA的以下金属除去。通过与单步浸出方法分别与单一HCl或单一EDTA的一步浸出方法进行了进一步证实了便利化。这些结果表明,HCl和EDTA的设计的两步浸出方法可用于选择性浸出和从冶金污泥或重金属污染的固体介质的重金属的有效回收。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号