Porous TiAl alloys with different nominal powder compositions were fabricated through a cost-effective powder metallurgy (PM) approach by sintering TiH2 and Al mixed powders. It is found that the pore properties vary with the TiH2 and Al contents, i.e., the nature of the pores can be improved by using different compositions. Furthermore, by detailed structural characterizations, four crystalline phases, i.e., alpha(2)-Ti3Al, TiAl3, and Ti2Al5, were observed in the fabricated porous TiAl alloys with different compositions. An optimal composition of TiH2-50wt% Al is preferred since its maximum open porosity is about 70% and its viscous permeability coefficient for nitrogen is 1.11 mu m(2). (C) 2015 Elsevier B.V. All rights reserved.
机译:通过烧结TiH2和Al混合粉末,通过具有成本效益的粉末冶金(PM)方法,制造了具有不同标称粉末成分的多孔TiAl合金。已经发现,孔的性质随TiH 2和Al的含量而变化,即,孔的性质可以通过使用不同的组成来改善。此外,通过详细的结构表征,在制备的具有不同组成的多孔TiAl合金中观察到四个晶相,即α(2)-Ti3Al,TiAl3和Ti2Al5。优选TiH2-50wt%Al的最佳组成,因为其最大开孔孔隙率约为70%,其对氮的粘滞渗透系数为1.11μm(2)。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号