The waste Nd-Fe-B sintered magnets up to 500 kg per batch were recycled to manufacture anisotropic sintered magnets by combination of hydrogen decrepitation (HD) and alloying technique. Magnetic properties and thermal stability of both the waste magnets and recycled magnets were investigated. The recycled magnet exhibits magnetic properties with remanence (B-r) of 12.38 kGs, coercivity (H-ci) of 24.89 kOe, and maximum energy product [(BH)(max)] of 36.51 MGOe, respectively, which restores 99.20% of B-r, 105.65% of H-ci, and 98.65% of (BH)(max) of the waste magnets, respectively. The volume fraction of Nd-rich phase in the recycled magnets is about 10.1 vol.%, which is bigger than that of the waste magnets due to the additive of Nd3PrFe14B alloy containing more rare earth. The remanence temperature coefficient (alpha) and coercivity temperature coefficient (beta) of the recycled magnets are -0.1155%/K and -0.5099%/K in the range of 288-423 K, respectively, which are comparative to those of the waste magnets. (C) 2015 Elsevier B.V. All rights reserved.
机译:每批重达500 kg的废Nd-Fe-B烧结磁体被回收利用,通过氢爆破(HD)和合金化技术相结合,制造出各向异性的烧结磁体。研究了废磁铁和再生磁铁的磁性能和热稳定性。再生磁体的磁性能分别为:剩磁(Br)为12.38 kGs,矫顽力(H-ci)为24.89 kOe,最大能量乘积[(BH)(max)]为36.51 MGOe,可还原99.20%的Br, H-ci的105.65%和废磁铁的(BH)(max)的98.65%。回收磁铁中富Nd相的体积分数约为10.1 vol。%,这比废磁铁大,这是由于Nd3PrFe14B合金中稀土含量更高所致。在288-423 K范围内,再生磁铁的剩磁温度系数α和矫顽力温度系数β分别为-0.1155%/ K和-0.5099%/ K,与废磁铁的相比。 (C)2015 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号