The effect of devulcanization level on mechanical properties of reclaimed rubber by thermal-mechanical shearing devulcanization

机译:脱硫水平对热机械剪切脱硫对再生橡胶力学性能的影响

获取原文
获取原文并翻译 | 示例
获取外文期刊封面目录资料

摘要

Ground tire rubber (GTR) with crosslinked structure has hardly any plasticity and processability, which makes its property very poor. Thermal-mechanical shearing devulcanization method can effectively destroy the crosslinked structure and restore GTR a certain extent of plasticity and processability. This article investigated the characteristic and reprocessing performance of reclaimed rubber prepared through thermal-mechanical shearing devulcanization. The relationship between the devulcanization level (indicated by gel fraction and crosslink density) and the mechanical property was analyzed by sufficient experiments. Fourier transform infrared spectroscopy and elemental analyzer studies revealed the chemical structure of GTR changed and many complex reactions occurred after devulcanization. The gel permeation chromatography indicated the specific changes of molecular weight and molecular weight distribution in devulcanization process. The differential scanning calorimetry revealed various vulcanized abilities and vulcanized structures of reclaimed rubber. The scanning electron microscope further confirmed the recovery of plasticity after devulcanization and the distinct vulcanized structures between revulcanizates. The determination of devulcanization level and mechanical properties verified that mechanical properties especially tensile strength reached to the optimum value only at an appropriate devulcanization level.
机译:具有交联结构的接地轮胎橡胶(GTR)几乎没有任何可塑性和可加工性,这使其性能非常差。热机械剪切脱硫方法可以有效破坏交联结构,并在一定程度上恢复GTR的可塑性和加工性。本文研究了热机械剪切脱硫制备的再生橡胶的特性和后处理性能。通过足够的实验分析了脱硫水平(由凝胶分数和交联密度表示)与机械性能之间的关系。傅里叶变换红外光谱和元素分析仪研究表明,脱硫后GTR的化学结构发生了变化,发生了许多复杂的反应。凝胶渗透色谱法表明了脱硫过程中分子量和分子量分布的特定变化。差示扫描量热法显示了再生橡胶的各种硫化能力和硫化结构。扫描电子显微镜进一步证实了脱硫后可塑性的恢复以及硫化橡胶之间明显的硫化结构。脱硫水平和机械性能的确定证明,只有在适当的脱硫水平下,机械性能,尤其是拉伸强度才达到最佳值。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号