Acrylonitrile-ammonium itaconate copolymers were prepared by H2O/dimethyl formamide suspension polymerization technique. Differential scanning calorimetry results of the degradation of acrylonitrile-ammonium itaconate copolymers in air are presented. The apparent activation energy of degradation of the copolymer was calculated using the Kissinger method. Effects of copolymerization conditions on the apparent activation energy of copolymer were studied. Increasing the dimethyl formamide concentration in the solvent mixture leads to a rapid increase in the degradation apparent activation energy of acrylonitrile-ammonium itaconate copolymer. The value of the degradation apparent activation energy of the copoly-mer synthesized in dimethyl formamide solvent increases up to 168.3 kJ mol(-1). The apparent activation energy decreases quickly along with an increase in ammonium itaconate concentration, and this change becomes less prominent as the weight ratio of ammonium itaconate/acrylonitrile goes beyond 6/94, Delta E-a = 89.4 +/- 2.0 kJ mol. The apparent activation energy shows a trend of increase with increasing copolymerization temperature. (c) 2005 Wiley Periodicals, Inc.
机译:采用H2O /二甲基甲酰胺悬浮聚合技术制备了丙烯腈-衣康酸铵共聚物。给出了在空气中降解丙烯腈-衣康酸铵共聚物的差示扫描量热法结果。使用基辛格方法计算共聚物降解的表观活化能。研究了共聚条件对共聚物表观活化能的影响。溶剂混合物中二甲基甲酰胺浓度的增加导致丙烯腈-衣康酸铵共聚物的降解表观活化能迅速增加。在二甲基甲酰胺溶剂中合成的共聚聚合物的降解表观活化能值增加到168.3 kJ mol(-1)。表观活化能随着衣康酸铵浓度的增加而迅速降低,并且随着衣康酸铵/丙烯腈的重量比超过6/94,ΔE-a = 89.4 +/- 2.0 kJ mol,这种变化变得不那么明显。表观活化能显示出随着共聚温度升高而增加的趋势。 (c)2005年Wiley Periodicals,Inc.

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号