The objective of this study is to compare the performances of catalytic ozonation processes of two activated carbons prepared from olive stone (ACOS) and apricot stone (ACAS) with commercial ones (granular activated carbon-GAC and powder activated carbon-PAC) in degradation of reactive azo dye (Reactive Red 195). The optimum conditions (solution pH and amount of catalyst) were investigated by using absorbencies at 532, 220 and 280 nm wavelengths. Pore properties of the activated carbon (AC) such as BET surface area, pore volume, pore size distribution, and pore diameter were characterized by N _2 adsorption. The highest BET surface area carbon (1,275 m ~2/g) was obtained from ACOS with a particle size of 2.29 nm. After 2 min of catalytic ozonation, decolorization performances of ACOS and ACAS (90.4 and 91.3%, respectively) were better than that of GAC and PAC (84.6 and 81.2%, respectively). Experimental results showed that production of porous ACs with high surface area from olive and apricot stones is feasible in Turkey.
机译:这项研究的目的是比较两种由橄榄石(ACOS)和杏石(ACAS)制成的活性炭与市售的活性炭(颗粒活性炭-GAC和粉末活性炭-PAC)的催化臭氧化工艺的性能。活性偶氮染料(活性红195)。通过使用在532、220和280 nm波长处的吸光度研究了最佳条件(溶液的pH和催化剂的量)。用N _2吸附表征了活性炭(AC)的孔隙性质,如BET表面积,孔体积,孔径分布和孔径。从ACOS获得最大的BET表面积碳(1,275 m〜2 / g),粒径为2.29 nm。催化臭氧化2分钟后,ACOS和ACAS的脱色性能(分别为90.4和91.3%)优于GAC和PAC(分别为84.6和81.2%)。实验结果表明,用橄榄石和杏石生产高表面积的多孔AC在土耳其是可行的。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号