Fabrication of manganese dioxide/carbon/attapulgite composites derived from spent bleaching earth for adsorption of Pb(II) and Brilliant green

机译:废漂白土衍生的二氧化锰/碳/凹凸棒石复合材料的制备,用于吸附Pb(II)和亮绿

获取原文
获取原文并翻译 | 示例
           

摘要

Manganese dioxide/carbon/attapulgite ternary composites were fabricated via a facile hydrothermal method based on spent bleaching earth. It is worth noting that the residual organic matter of the spent bleaching earth not only served as a low-cost available carbon precursor, but also as a reductant for the formation of manganese dioxide based on the redox with KMnO4. Using the organic dye of Brilliant green and the heavy metal ion of Pb(II) as model pollutants, the effect of the critical factors on the adsorption properties have been systematically investigated, including the sample preparation conditions, contact time and initial concentration of pollutants. The results reveal that the adsorption properties of the as-prepared composites are well dependent on the concentration of KMnO4, and the maximum adsorption capacity toward Brilliant green and Pb(II) can reach 199.99 mg g(-1) and 166.64 mg g(-1) while the concentration of KMnO4 is 12% and 16%, respectively.
机译:二氧化锰/碳/凹凸棒三元复合材料是通过基于废漂白土的简便水热法制备的。值得注意的是,废漂白土中的残留有机物不仅可以用作低成本的可用碳前体,而且还可以作为还原剂,用于在以KMnO4氧化还原的基础上形成二氧化锰。以亮绿色有机染料和Pb(II)的重金属离子为模型污染物,系统地研究了关键因素对吸附性能的影响,包括样品的制备条件,接触时间和污染物的初始浓度。结果表明,所制备的复合材料的吸附性能与KMnO4的浓度密切相关,对亮绿和Pb(II)的最大吸附能力可以达到199.99 mg g(-1)和166.64 mg g(- 1)而KMnO4的浓度分别为12%和16%。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号