Na-ion batteries (NIB) are now attracting researchers' attention as possible substitutes of Li-ion batteries. Promising cathode materials, which have demonstrated to work well for NIB are those based on the sodiated Prussian Blue, NaFeFe(CN)(6), Prussian White, Na2FeFe(CN)(6), and their analogues. Herein, the effect of different electrolytes and binder composition, on the electrochemical performance of sodium Prussian Blue, Na0.75Fe2.08(CN)(6)center dot 3.4H(2)O, as cathode material for NIB is studied. Several electrolytes containing NaClO4 or NaPF6 salts in carbonated mixtures, with and without fluoroethylene carbonate (FEC) as additive, have been tested for Na0.75Fe2.08(CN)(6)center dot 3.4H(2)O. The effect of different binders, polyvinylidene fluoride (PvdF), sodium carboxymethyl cellulose (CMC), polytetrafluoroethylene (PTFE) and ethylene propylene diene monomer ruber (EPDM), is also investigated. (C) 2016 Elsevier Ltd. All rights reserved.
机译:钠离子电池(NIB)作为锂离子电池的替代品正在引起研究人员的关注。已证明对NIB很好的阴极材料是基于普鲁士蓝,NaFeFe(CN)(6),普鲁士白,Na2FeFe(CN)(6)及其类似物的阴极材料。在这里,研究了不同的电解质和粘合剂组成对普鲁士蓝钠Na0.75Fe2.08(CN)(6)中心点3.4H(2)O作为NIB正极材料的电化学性能的影响。已测试了几种含碳酸钠混合物中的NaClO4或NaPF6盐的电解质,有无氟碳酸亚乙酯(FEC)作为添加剂,对Na0.75Fe2.08(CN)(6)中心点3.4H(2)O进行了测试。还研究了不同粘合剂,聚偏二氟乙烯(PvdF),羧甲基纤维素钠(CMC),聚四氟乙烯(PTFE)和乙丙二烯单体橡胶(EPDM)的效果。 (C)2016 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号