Na-deficient O3-type materials Na0.8Ni0.4-xCo2xTi0.6-xO2 (x = 0, 0.05, 0.1, and 0.15) were synthesized by a simple solid-state reaction and investigated as cathode materials for room-temperature sodium-ion batteries. Among these materials, O3-Na0.8Ni0.3Co0.2Ti0.5O2 exhibits excellent cycle stability and good rate capability. It delivers an initial capacity of 84 mAh/g in the voltage range of 2.5-4.2V at a current rate of 0.1 degrees C. Approximately 95% of the capacity is maintained after 90 cycles, and the Coulombic efficiency reaches nearly 99% after the initial cycles. At a current rate of 1 degrees C, the capacity retention is 81% of the initial capacity. These results indicate that Co-substitution can improve the cycle stability during the course of sodium extraction and insertion. (C) 2015 Elsevier Ltd. All rights reserved.
机译:通过简单的固相反应合成了Na缺乏的O3型材料Na0.8Ni0.4-xCo2xTi0.6-xO2(x = 0、0.05、0.1和0.15),并将其用作室温钠离子的阴极材料。离子电池。在这些材料中,O3-Na0.8Ni0.3Co0.2Ti0.5O2具有出色的循环稳定性和良好的倍率性能。它以0.1摄氏度的电流速率在2.5-4.2V的电压范围内提供84 mAh / g的初始容量。在90次循环后,大约95%的容量得以保持,而在90循环后,库仑效率达到近99%。初始周期。在1摄氏度的电流速率下,容量保持率为初始容量的81%。这些结果表明,共取代可以改善钠提取和插入过程中的循环稳定性。 (C)2015 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号