摘要

Upconversion La2,(MoO.,)1:Eu~(3+)/Yb~(3+) phosphors with doping concentrations of Ei~(3+) and Yb~(3+) (x = Er~(3+) + Yb~(3+), Er~(3+) = 0.05, 0.1, 0.2 and Yb~(3+) = 0.2,0.45) were successfully synthesized by the cyclic microwave-assisted sol-gel process and the upconversion photoluminescence properties have been investigated. Well-crystallized particles, formed after heat-treatment at 900 °C for 16 h, showed a fine and homogeneous morphology with particle sizes of 1-5 um. Under excitation at 980 nm, La_(1.7)(MoO4)3.Er_(0.1)Yb_(0.2) and Lai.5(MoQ4)3:Er_(0.05)Yb_(0.45) particles exhibited a strong 525 nm emission band, a weak 550 nm emission band in the green region and a very weak 655 nm emission band in the red region. The Raman spectra of the particles indicated the presence of weak peaks at lower frequencies induced by the disorder of the [MoO4]~3 groups with the incorporation of the Er~(3+) and Yb~(3+) elements into the crystal lattice or by a new phase formation.
机译:掺杂浓度为Ei〜(3+)和Yb〜(3+)的上转换La2,(MoO。,)1:Eu〜(3 +)/ Yb〜(3+)荧光粉(x = Er〜(3+)通过循环微波辅助溶胶-凝胶法和上转换光致发光性能成功合成了+ Yb〜(3 +),Er〜(3+)= 0.05、0.1、0.2和Yb〜(3+)= 0.2、0.45)已被调查。在900°C热处理16小时后形成的结晶良好的颗粒,显示出细微且均匀的形貌,粒径为1-5微米。在980 nm激发下,La_(1.7)(MoO4)3.Er_(0.1)Yb_(0.2)和Lai.5(MoQ4)3:Er_(0.05)Yb_(0.45)粒子表现出很强的525 nm发射带,绿色区域的550 nm发射带很弱,红色区域的655 nm发射带很弱。粒子的拉曼光谱表明,[MoO4]〜3基团的无序性导致了低频下弱峰的出现,其中Er〜(3+)和Yb〜(3+)元素掺入了晶格或通过新的阶段形成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号