The effects of Fe(II) and Fe(III) concentration and initial pH on microbial leaching of low-grade sphalerite ore in a column reactor

机译:Fe(II)和Fe(III)的浓度以及初始pH对柱式反应器中低品位闪锌矿矿石微生物浸出的影响

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

In this study the effects of initial concentration of Fe(II) and Fe(III) ions as well as initial pH on the bioleaching of a low-grade sphalerite ore in a leaching column over a period of 120 days with and without bacteria were investigated. Four different modifications of medium were used as column feed solutions to investigate the effects of initial concentration of Fe(II) and Fe(III) ions on zinc extraction. The experiments were carried out using a bench-scale, column leaching reactor, which was inoculated with mesophilic iron oxidizing bacteria, Acidithiobacillus ferrooxidans, initially isolated from the Sarcheshmeh chalcopyrite concentrate (Kerman, Iran). The effluent solutions were periodically analyzed for Zn, total Fe, Fe(II) and Fe(III) concentrations as well as pH values. Bacterial population was measured in the solution (free cells). Maximum zinc recovery in the column was achieved about 76% using medium free of initial ferrous ion and 11.4 g/L of ferric ion (medium 2) at pH 1.5. The extent of leaching of sphalerite ore with bacteria was significantly higher than that without bacteria (control) in the presence of ferrous ions. Fe(III) had a strong influence in zinc extraction, and did not adversely affect the growth of the bacteria population. (c) 2007 Elsevier Ltd. All rights reserved.
机译:在这项研究中,研究了Fe(II)和Fe(III)离子的初始浓度以及初始pH对120天内有无细菌的浸出柱中低品位闪锌矿矿石生物浸出的影响。 。使用四种不同的培养基作为色谱柱进料溶液,以研究初始浓度的Fe(II)和Fe(III)离子对锌提取的影响。实验是使用台式规模的柱浸反应器进行的,该反应器接种了嗜温铁氧化细菌,铁氧化酸硫硫杆菌,最初从Sarcheshmeh黄铜矿精矿中分离出来(伊朗,德国)。定期分析废水溶液中的Zn,总Fe,Fe(II)和Fe(III)浓度以及pH值。测量溶液(游离细胞)中的细菌种群。使用不含初始亚铁离子和11.4 g / L三价铁离子(介质2)的pH值为1.5的色谱柱,锌的最大回收率约为76%。存在亚铁离子时,有细菌的闪锌矿浸出程度明显高于无细菌的浸出程度(对照)。 Fe(III)对锌的提取有很大影响,并且对细菌种群的生长没有不利影响。 (c)2007 Elsevier Ltd.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号