The extensional properties of 2-hydroxypropyl ether guar gum solutions were investigated using a capillary breakup extensional rheometer (CaBER). Optimization of the geometric parameters of this device allowed for the measurement of the characteristic relaxation times and the apparent extensional viscosities of a series of dilute to semidilute guar gum solutions. The measured relaxation times were compared with predicted Zimm relaxation times, assuming that the hydrophobically modified guar was in a good solvent. Good agreement was found at low concentrations (0.01 wt % ≈ 0.17c~*, where c~* is the polymer overlap concentration), and this technique allowed for relaxation times on the order of 1 ms to be measured for solutions with shear viscosities of 2 mPa· s. Both the shear and (apparent) steady-state extensional viscosities of this set of industrially relevant fluids exhibited two regions of dependency on polymer concentration: linear up to concentrations of 0.2 wt % (c/c~* ≈ 3) and power law thereafter, where interchain interactions became significant. The extracted relaxation times followed the same trend (i.e., having a near linear dependency on concentration up to 0.2 wt % and a power-law dependency on concentration up to 9c~*). The results indicate that the transition from dilute to semidilute behavior occurs at a nominal concentration of ~3c~* instead of c~*. The results presented suggest that interchain interactions for this modified guar are weak overall, and the solutions investigated are absent of entanglements over the whole range of frequencies and concentrations explored ((0.17—9)c~*).
机译:使用毛细管破裂延伸流变仪(CaBER)研究了2-羟丙基醚瓜尔胶溶液的延伸特性。该装置的几何参数的优化允许测量一系列稀至半稀瓜尔胶溶液的特征驰豫时间和表观延伸粘度。假定疏水改性的瓜尔胶处于良好溶剂中,则将测得的弛豫时间与预测的Zimm弛豫时间进行比较。在低浓度(0.01 wt%≈0.17c〜*,其中c〜*为聚合物重叠浓度)下发现良好的一致性,对于剪切粘度为1的溶液,该技术可以测量1 ms左右的松弛时间。 2兆帕·秒。这套与工业相关的流体的剪切和(表观)稳态拉伸粘度都表现出两个取决于聚合物浓度的区域:线性直至浓度为0.2 wt%(c / c〜*≈3)以及此后的幂律,链间互动变得很重要。所提取的弛豫时间遵循相同的趋势(即,对浓度至多0.2wt%具有近乎线性的依赖性,对浓度至多9c- *具有幂律的依赖性)。结果表明,从稀行为到半稀行为的转变发生在〜3c〜*的名义浓度而不是c〜*。提出的结果表明,该修饰瓜耳胶的链间相互作用总体上较弱,并且在所研究的整个频率和浓度范围内((0.17-9)c〜*)都没有纠缠的解决方案。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号