Promotion of H2O2 decomposition activity over beta-MnO2 nanorod catalysts

机译:通过β-MnO2纳米棒催化剂促进H2O2分解活性

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

The relationship among the beta-MnO2 nanorod preparation conditions, morphology and catalytic performance on H2O2 decomposition has been investigated in the work. beta-MnO2 nanorod catalysts were prepared by heating different gamma-MnOOH nanorod precursors at 250-450 degrees C. They were characterized by X-ray diffraction (XRD), transmission electron microscopy (TEM) and nitrogen adsorption. The experimental results indicate that gamma-MnOOH nanorod precursors prepared at higher hydrothermal temperature make final beta-MnO2 nanorods uniform. The catalytic performance on H2O2 decomposition shows that beta-MnO2 nanorod catalysts have excellent catalytic activity on the decomposition of H2O2, which has not been reported to our knowledge. beta-MnO2 nanorods which were prepared by calcining gamma-MnOOH precursors at 250 C have higher catalytic activity than those at higher calcination temperatures. The reaction of H2O2 decomposition over beta-MnO2 nanorod catalysts was found to follow first-order kinetics. (c) 2007 Elsevier B.V. All rights reserved.
机译:研究了β-MnO2纳米棒制备条件,形态和催化性能对H2O2分解之间的关系。 β-MnO2纳米棒催化剂是通过在250-450℃下加热不同的γ-MnOOH纳米棒前体制备的。它们的特征在于X射线衍射(XRD),透射电子显微镜(TEM)和氮吸附。实验结果表明,在较高的水热温度下制备的γ-MnOOH纳米棒前体使最终的β-MnO2纳米棒均匀。 H 2 O 2分解的催化性能表明,β-MnO2纳米棒催化剂对H 2 O 2的分解具有优异的催化活性,据我们所知尚未报道。通过在250°C下煅烧γ-MnOOH前体制备的β-MnO2纳米棒比在较高煅烧温度下具有更高的催化活性。发现在β-MnO2纳米棒催化剂上H2O2分解的反应遵循一级动力学。 (c)2007 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号