首页> 外文期刊>Colloids and Surfaces, A. Physicochemical and Engineering Aspects >Novel amphiphilic triblock copolymer based on PPDO, PCL, and PEG: Synthesis, characterization, and aqueous dispersion
【24h】

Novel amphiphilic triblock copolymer based on PPDO, PCL, and PEG: Synthesis, characterization, and aqueous dispersion

机译:基于PPDO,PCL和PEG的新型两亲三嵌段共聚物:合成,表征和水分散体

获取原文
获取原文并翻译 | 示例
           

摘要

Amphiphilic triblock copolymer, poly(p-dioxanone-co-caprolactone)-block-poly(ethylene oxide)-block-poly(p-dioxanone-co-caprolactone) (PPDO-co-PCL-b-PEO-b-PPDO-co-PCL) was synthesized by ring opening polymerization (ROP) of p-dioxanone and epsilon-caprolactone initiated through the hydroxyl end of poly(ethylene glycol) (PEG) in the presence of stannous 2-ethyl hexanoate [Sn(oct)(2)] as a catalyst. Polymerization and structural features of the polymers were analyzed by different physicochemical techniques (GPC, H-1 NMR, C-13 NMR, FT-IR, DSC and TGA). The splitting of H-1 NMR resonance at delta 2.3 and delta 4.1 ppm reveals the random copolymerization. Polymeric nanoparticles were prepared in phosphate buffer (pH 7.4) by co-solvent evaporation technique at room temperature (25 degrees C). Existence of hydrophobic domains as cores of the micelles were characterized by 1 H NMR spectroscopy and further confirmed with fluorescence technique using pyrene as a probe. Critical micelle concentration (CMC) of the polymer in phosphate buffer (pH. 7.4) was decreased from 2.3 x 10(-3) to 7.6 x 10(-4) g/L with the fraction of PCL. Polymeric nanoparticles observed by atomic force microscopy (AFM) were uniform and spherical, with smooth textured of around 50-30 nnn diameter. Dynamic light scattering (DLS) and electrophoretic light scattering (ELS) measurements showed a monodisperse size distribution of around 113-90 nm hydrodynamic diameters and negative zeta (xi) potential (-4 to - 14 mV), respectively. The investigations for the polymeric nanoparticles in aqueous medium showed that the composition of the hydrophobic segment of amphiphilic block copolymer makes a significant influence on its physicochemical characteristics. (c) 2006 Elsevier B.V. All rights reserved.
机译:两亲性三嵌段共聚物,聚(对-二恶烷酮-己内酯)-嵌段-聚(环氧乙烷)-嵌段-聚(对二恶烷酮-己内酯)(PPDO-co-PCL-b-PEO-b-PPDO- co-PCL)是通过在己酸2-乙基亚锡(Sn(oct)()的存在下,通过聚乙二醇(PEG)的羟基端引发的对二恶烷酮和ε-己内酯的开环聚合(ROP)合成的2)]作催化剂。通过不同的物理化学技术(GPC,H-1 NMR,C-13 NMR,FT-IR,DSC和TGA)分析了聚合物的聚合和结构特征。 H-1 NMR共振在δ2.3和δ4.1 ppm处的分裂表明无规共聚。在室温(25摄氏度)下通过共溶剂蒸发技术在磷酸盐缓冲液(pH 7.4)中制备聚合物纳米颗粒。通过1 H NMR光谱表征疏水域作为胶束核心的存在,并进一步使用pyr作为探针通过荧光技术确认。聚合物在磷酸盐缓冲液(pH 7.4)中的临界胶束浓度(CMC)从2.3 x 10(-3)g / L降低到7.6 x 10(-4)g / L(PCL的分数)。通过原子力显微镜(AFM)观察到的聚合物纳米粒子是均匀且球形的,具有约50-30 nnn直径的光滑纹理。动态光散射(DLS)和电泳光散射(ELS)测量表明,流体动力学直径的单分散尺寸分布约为113-90 nm,负电动势(xi)为(-4至-14 mV)。在水性介质中对聚合物纳米粒子的研究表明,两亲性嵌段共聚物的疏水链段的组成对其物理化学特性有重要影响。 (c)2006 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号