Fine composite particles containing yttrium and ironwere prepared from homogeneous solution using urea as aprecipitant generator. The ratio of yttrium to iron in the precipitatecould be controlled by adjusting the concentration of the startingmaterials in the initial solution. These composite particles wereconsidered to be amorphous. Shapes and morphology of theprecipitated particles were influenced by the difference of thereaction conditions. Particles obtained from the solutioncontaining 1.88mmol dm-3 FeCl3·6H2O, 3.13mmol dm-3YCl3·6H2O and 500mmol dm-3 urea at 97℃were almost sphericaland mono-dispersed, Particles precipitated on the condition asmentioned above converted from amorphous into monophasicgarnet (Y3Fe5O12) by calcining at 1,200℃ for 5 hours. Aftercalcination, particle changed its color from brown to mediumolive and indicated marked magnetic character.
机译:使用尿素作为沉淀剂,从均相溶液中制备出含有钇和铁的复合微粒。沉淀物中钇与铁的比例可以通过调节初始溶液中原料的浓度来控制。这些复合颗粒被认为是无定形的。反应条件的不同会影响沉淀颗粒的形状和形貌。在97℃下,由1.88mmol dm-3 FeCl3·6H2O,3.13mmol dm-3YCl3·6H2O和500mmol dm-3尿素制成的溶液几乎呈球形和单分散。 Y3Fe5O12)在1200℃煅烧5小时。煅烧后,颗粒的颜色从棕色变为中等橄榄色,并显示出明显的磁性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号