Various modified silica sorbents and unmodified silica were tested for the separation and preconcentration of 10-200 ng cm~(-3) from 50-1 000 cm~3 sample volume of platinum group metals (PGMs), Pt(IV, II), Pd(II), Ir(IV), Rh(III), Os(VI), Ru(IV) and Au(III) in the form of ion associates of their chloro and bromo complexes with cationic surfactants. [l-(Ethoxy-carbonyl)pentadecyl]trimethylammonium bromide (Septonex~R), benzyl(dodecyl)dimethyl-ammonium bromide (Sterinol~R), trimethyl(tetradecyl)ammonium bromide or hexadecyl(trimethyl)arnmonium chloride and 0.1 m HC1 or 0.1 m HBr are suitable for the purpose. 100% recovery for Pd(II), Pt(IV) and Au(III) was obtained with octadecyl silicas Separon~(TM) SGX C18, Separon~(TM) SGX RPS and Phenyl~(TM) silica in the presence of 0.006 M Septonex~R or 0.003 m Sterinol~R. The retained PGMs and Au(III) were eluted with acetonitrile and determined by inductively coupled plasma atomic emission spectrometry (ICP-AES) after evaporation of organic solvent in the presence of 0.1 m HC1. The enrichment factor on Separon~(TM) SGX RPS reaches 100. A 1 000 : 1 excess of Cl~-, NO_3~-, SO_4~(2-), Na~+, K~+, Ca~(2+), Mg~(2+), Fe~(3+) or Al~(3+) does not interfere with the preconcentration of PGMs and Au(III) on this sorbent. With the silica-based anion exchanger Separon~(TM) SGX AX, the 100% recovery is observed for Ir(IV), Pd(II), Pt(IV) when the elution is performed with 5 m HC1 or 5 m HNO_3. Macroporous sorbents Amberlite~(TM) XAD2 and Amberlite~(TM) XAD4 are suitable for the retention of Au(III), Pd(II) and Pt(IV) from 0.1 m HC1 and 0.006 m Septonex~R. 100% recovery is achieved using acetonitrile as eluent but there is no preference of these sorbents to modified silica. In this way, the recovery of 0.1-0.2 (mu)g cm~(-3) Au(III), Pd(II), Pt(IV) was also successfully tested with spiked matrices of soil extracts, power station dust samples and natural waters.
机译:测试了各种改性二氧化硅吸附剂和未改性二氧化硅对铂族金属(PGM),Pt(IV,II),50-1 000 cm〜3样品体积中10-200 ng cm〜(-3)的分离和预富集, Pd(II),Ir(IV),Rh(III),Os(VI),Ru(IV)和Au(III)以其氯和溴配合物与阳离子表面活性剂的离子缔合形式存在。 [1-(乙氧羰基)十五烷基]三甲基溴化铵(Septonex〜R),苄基(十二烷基)二甲基溴化铵(Sterinol〜R),三甲基(十四烷基)溴化铵或十六烷基(三甲基)氯化铵和0.1 m HCl或0.1 m HBr适用于此目的。用十八烷基二氧化硅SeparonTM SGX C18,SeparonTM SGX RPS和苯基TM二氧化硅在0.006的存在下获得100%的Pd(II),Pt(IV)和Au(III)回收率。 M Septonex〜R或0.003 m Sterinol〜R。在0.1 m HCl存在下蒸发有机溶剂后,用乙腈洗脱保留的PGM和Au(III),并通过电感耦合等离子体原子发射光谱法(ICP-AES)测定。 Separon〜(TM)SGX RPS的富集因子达到100。Cl〜-,NO_3〜-,SO_4〜(2-),Na〜+,K〜+,Ca〜(2+)的比例为1000:1。 ,Mg〜(2 +),Fe〜(3+)或Al〜(3+)不会干扰PGM和Au(III)在该吸附剂上的预富集。使用二氧化硅基阴离子交换剂SeparonTM SGX AX,当用5 m HCl或5 m HNO_3洗脱时,观察到Ir(IV),Pd(II),Pt(IV)的100%回收率。大孔吸附剂AmberliteTM XAD2和AmberliteTM XAD4适用于从0.1 m HCl和0.006 m Septonex〜R中保留Au(III),Pd(II)和Pt(IV)。使用乙腈作为洗脱液可实现100%的回收率,但这些吸附剂并不比改性硅胶好。通过这种方式,还成功地利用掺入的土壤提取物,发电厂粉尘样品和污染物的基质测试了0.1-0.2μgcm〜(-3)Au(III),Pd(II),Pt(IV)的回收率。天然水域。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号