A series of catalysts of Ag2O-Co3O4/gamma-Al2O3 was prepared by equivalent volume impregnation method. The effects of the metal loading, calcination time, and calcination temperatures of Ag and Co, respectively, on the catalytic activity were investigated. The optimum preparing condition of Ag2O-Co(3)O4/gamma-Al2O3 was decided, and then the influence of different preparation conditions on catalytic activity of Ag2O-Co3O4/gamma-Al2O3 was analyzed. The results showed the following: (1) at the same preparation condition, when silver loading was 8%, the Ag2O-Co3O4/gamma-Al2O3 showed higher catalyst activity, (2) the catalyst activity had obviously improved when the cobalt loading was 8%, while it was weaker at loadings 5% and 10%, (3) the catalyst activity was influenced by different calcination temperatures of silver, but the influences were not marked, (4) the catalyst activity can be influenced by calcination time of silver, (5) different calcination times of cobalt can also influence the catalyst activity of Ag2O-Co3O4/gamma-Al2O3, and (6) the best preparation conditions of the Ag2O-Co3O4/gamma-Al2O3 were silver loading of 8%, calcination temperature of silver of 450 degrees C, and calcinations time of silver of 4 h, while at the same time the cobalt loading was 8%, the calcination temperature of cobalt was 450 degrees C, and calcination time of cobalt was 4 h.
机译:通过等体积浸渍法制备了一系列Ag2O-Co3O4 /γ-Al2O3催化剂。研究了金属负载量,煅烧时间和Ag和Co的煅烧温度对催化活性的影响。确定了Ag2O-Co(3)O4 /γ-Al2O3的最佳制备条件,然后分析了不同制备条件对Ag2O-Co3O4 /γ-Al2O3催化活性的影响。结果表明:(1)在相同的制备条件下,当载银量为8%时,Ag2O-Co3O4 /γ-Al2O3具有较高的催化剂活性;(2)当钴载量为8时,催化剂活性明显提高。 %,尽管在5%和10%的负载下较弱,(3)催化剂活性受银的不同煅烧温度的影响,但没有显着影响,(4)催化剂活性受银的煅烧时间的影响,(5)钴的不同煅烧时间也会影响Ag2O-Co3O4 /γ-Al2O3的催化剂活性,(6)Ag2O-Co3O4 /γ-Al2O3的最佳制备条件是载银量为8%,煅烧温度在450℃的温度下,银的煅烧时间为4h,同时钴的负载量为8%,钴的煅烧温度为450℃,钴的煅烧时间为4h。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号