In order to improve copper leaching efficiency from the flexible printed circuit board (PCB) by Acidithiobacillus ferrooxidans, it is necessary to quantitatively measure the bacteria bioleaching copper under extreme acidic condition from flexible PCB. The inductively coupled plasma-atomic emission spectroscopy (ICP-AES) is a very accurate way to analyze metals in solution; this paper investigated the optimal conditions for copper bioleaching by Acidithiobacillus ferrooxidans from flexible PCB through ICP-AES. The conditions included particle size of flexible PCB powder, quantity of flexible PCB powder, initial pH of culture medium, bacteria inoculation, bacteria activation time, and quantity of FeSO4 center dot 7H(2)O. Prior to ICP-AES measurement, culture solution was digested by aqua regia. The experimental results demonstrated that flexible PCB contained one main metal (copper); this was associated with the structure of flexible PCB. The optimization conditions were in 50 mL medium, flexible PCB 10 g/L, particle size of flexible PCB 0.42 similar to 0.84 mm, culture medium initial pH 2.5, bacteria inoculation 5%, bacteria activation time 5 d, and quantity of FeSO4 center dot 7H(2)O 30 g/L. Under the optimization condition, the leaching rate of copper was 90.10%, which was 42.4% higher than the blank group. For the ICP-AES determination, it reached a conclusion that the best corresponding wavelength (nm) of copper will be 224.7 (nm).
机译:为了提高酸性氧化硫硫杆菌从柔性印刷电路板(PCB)浸出铜的效率,有必要定量地测量在极端酸性条件下从柔性PCB浸出的细菌生物浸出铜的细菌。电感耦合等离子体原子发射光谱法(ICP-AES)是分析溶液中金属的非常准确的方法。本文研究了铁氧酸硫杆菌通过ICP-AES从柔性PCB浸出铜的最佳浸提条件。条件包括柔性PCB粉的粒径,柔性PCB粉的量,培养基的初始pH,细菌接种,细菌活化时间和FeSO4中心点7H(2)O的量。在进行ICP-AES测量之前,将王水消化培养液。实验结果表明,柔性PCB包含一种主要金属(铜);而另一种主要金属是铜。这与柔性PCB的结构有关。优化条件是在50 mL培养基,10 g / L的柔性PCB中,0.42的柔性PCB粒度类似于0.84 mm,培养基初始pH 2.5,细菌接种5%,细菌活化时间5 d和FeSO4中心点的数量7H(2)O 30克/升。在优化条件下,铜的浸出率为90.10%,比空白组高42.4%。对于ICP-AES测定,得出的结论是,铜的最佳对应波长(nm)为224.7(nm)。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号