The present scientific study focused on leaching behavior of uranium and vanadium from Korean domestic ore. The leaching process experimental conditions optimized for uranium and vanadium metals recovery from Korean domestic ore and developed the basic experimental procedures such as time, particle size, acid influence, temperature effect and pulp density (PD) behavior. Acid influence on leaching process was tested and noted that 2.0 M sulfuric acid concentration is the optimized conditions for present study. The time influence on leaching process was observed and its optimized 2 h for complete leaching process. The temperature influence tested and optimized the 80 ℃ for complete leaching process and PD is 50 %(wt%). The bench scale experiments developed in a laboratory and tested in pilot level each batch 100 kg of ore sample.
机译:目前的科学研究集中于从韩国国内矿石中浸出铀和钒的行为。优化了从韩国国产矿石中回收铀和钒金属的浸出工艺实验条件,并开发了基本的实验程序,例如时间,粒度,酸影响,温度效应和纸浆密度(PD)行为。测试了酸对浸出过程的影响,并指出2.0 M的硫酸浓度是本研究的最佳条件。观察了时间对浸出过程的影响,并优化了2小时以完成浸出过程。温度影响测试并优化了80℃,以完成浸出过程,PD为50%(wt%)。实验室规模试验是在实验室中开发的,并在中试水平下每批100千克矿石样品进行了测试。

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号