Random multiblock poly(ester amide)s containing poly (L-lactide) and cycloaliphatic amide segments: Synthesis and biodegradation studies

机译:包含聚(L-丙交酯)和脂环族酰胺链段的无规多嵌段聚(酯酰胺):合成和生物降解研究

获取原文
获取原文并翻译 | 示例
   

获取外文期刊封面封底 >>

       

摘要

Novel multiblock poly(ester amide)s containing poly(L-lactide) and cycloaliphatic amide segments were synthesized from telechelic oligomer of alpha,omega-hydroxyl terminated poly(L-lactide), 1,3-cyclohexylbis(methylamine), and sebacoylchloride by the "two-step" interfacial polycondensation method. The blocky nature of PEAs was established by FTIR and H-1 NMR spectroscopies. The effect of relative content of ester and amide segments on the crystallization nature of PEAs was investigated by WAXD and DSC analyses. PEAs having lower content of PLLA, PEA 1 and PEA 2, showed a crystallization pattern analogous to polyamides, whereas PEA 3, having higher content of PLLA, showed two crystalline phases characterized by polyester and polyamide segments. Random nature of PEAs was observed from single T-g values. Biodegradation studies using the enzyme lipase from Candida Cylindracea showed higher degradation rate for PEA 3 than that for PEA 1 and PEA 2. FTIR, 1(H) NMR, and DSC analyses of the degraded products indicated the involvement of ester linkages in the degradation process.
机译:由α,ω-羟基封端的聚(L-丙交酯),1,3-环己基双(甲胺)和癸二酰氯的远螯低聚物合成了包含聚L-丙交酯和脂环族酰胺链段的新型多嵌段聚(酯酰胺) “两步法”界面缩聚法。通过FTIR和H-1 NMR光谱确定了PEA的嵌段性质。通过WAXD和DSC分析,研究了酯和酰胺链段的相对含量对PEA结晶性质的影响。具有较低PLLA含量的PEA,PEA 1和PEA 2具有类似于聚酰胺的结晶模式,而具有较高PLLA含量的PEA 3具有以聚酯和聚酰胺链段为特征的两个结晶相。从单个T-g值观察到PEA的随机性质。使用假丝酵母念珠菌的脂肪酶进行的生物降解研究表明,PEA 3的降解速率高于PEA 1和PEA 2的降解速率。FTIR,1(H)NMR和DSC分析降解产物表明酯键参与降解过程。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号