Laccase was immobilised on polyethyleneglycol diacrylate (PEGDA) microspheres. The optimal preparation conditions of PEGDA microspheres were as follows: 3.0% (w/v) 2,2-azobisisobutyro-nitrite (AIBN), 4.0-5.0% (w/v) polyvinylpyrrolidone (PVP), 5.0-8.0% (w/v) glucose and 4.0% (w/v) PEGDA in glucose solution. The volume ratio of PEGDA solution, glucose/PVP solution and AIBN solution was 25: 100: 1. Microspheres obtained exhibited good characteristics with small sizes (1-4 mu m). The immobilised laccase showed a higher stability in a wide pH range. Thermal stability and storage stability of immobilised laccase were enhanced. The activity of immobilised laccase was 45.0% after six cycles uses. Only 62.7% of the activity remained for free laccase while there was a 60.4% increased for immobilised laccase with storage at 4 degrees C for 25 d. The K-m value of laccase increased from 21.9 to 114.0 mu mol/l after immobilisation.
机译:漆酶被固定在聚乙二醇二丙烯酸酯(PEGDA)微球上。 PEGDA微球的最佳制备条件如下:3.0%(w / v)2,2-偶氮二异丁腈-亚硝酸盐(AIBN),4.0-5.0%(w / v)聚乙烯吡咯烷酮(PVP),5.0-8.0%(w / v) v)葡萄糖溶液中的葡萄糖和4.0%(w / v)PEGDA。 PEGDA溶液,葡萄糖/ PVP溶液和AIBN溶液的体积比为25:100:1。获得的微球具有良好的特性,且具有小尺寸(1-4μm)。固定的漆酶在宽的pH范围内显示出更高的稳定性。固定化漆酶的热稳定性和储存稳定性得到增强。经过六次循环使用,固定化漆酶的活性为45.0%。游离漆酶仅保留62.7%的活性,而固定化漆酶在4°C下保存25 d则增加60.4%。固定后,漆酶的K-m值从21.9增加到114.0μmol/ l。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号