摘要

This paper reports on the results of four different wet chemical techniques used for the synthesis of superconducting oxides. YBa2Cu3O7 (YBCO). YBCO samples were prepared by complexion citric gel route (CT), acetate-tartrate sol-gel (ASG), oxalate/ethanol coprecipitation (COP), and acetate-tartrate sol-gel solid-state reaction (ASG-SSR) techniques. Each of the YBCO powders was annealed for 4 h at 880 degrees C, 900 degrees C, 920 degrees C, and 950 degrees C to find the optimum temperature. The optimum sintering temperature for the formation of Y-123 phase is very much dependent on the type of wet chemical technique used to prepare the powders. (C) 2008 Elsevier B.V. All rights reserved.
机译:本文报告了用于合成超导氧化物的四种不同的湿化学技术的结果。 YBa2Cu3O7(YBCO)。 YBCO样品是通过柠檬酸络合凝胶法(CT),乙酸盐-酒石酸盐溶胶-凝胶(ASG),草酸盐/乙醇共沉淀(COP)和乙酸盐-酒石酸盐溶胶-凝胶固态反应(ASG-SSR)技术制备的。将每种YBCO粉末在880摄氏度,900摄氏度,920摄氏度和950摄氏度下退火4小时,以找到最佳温度。 Y-123相形成的最佳烧结温度在很大程度上取决于用于制备粉末的湿化学技术的类型。 (C)2008 Elsevier B.V.保留所有权利。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号