Novel core-shell Fe3O4@poly(dopamine) magnetic nanoparticles were prepared through an in situ self-polymerization method. The hybrid nanomaterial showed an average core diameter of 11 ± 3 nm and a polymer thin film thickness of 1.8 ± 0.2 nm. The core-shell nanoparticles were employed as solid supports for the covalent immobilization of horseradish peroxidase (HRP), and the resulting biofunctionalized magnetic nanoparticles were employed to construct an amperometric biosensor for H2O2. The enzyme biosensor showed a high sensitivity of 442.14 mA M~(-1) cm~(-2), a low limit of detection of 182 nM, a wide linear range from 6.0 × 10~(-7) to 8.0 × 10~(-4) M and high stability for 1 month.
机译:通过原位自聚法制备了新型的核壳型Fe3O4 @聚(多巴胺)磁性纳米粒子。杂化纳米材料的平均芯直径为11±3 nm,聚合物薄膜厚度为1.8±0.2 nm。核-壳纳米粒子被用作共价固定辣根过氧化物酶(HRP)的固体载体,所得生物功能化的磁性纳米粒子被用于构建H2O2的安培生物传感器。该酶生物传感器具有442.14 mA M〜(-1)cm〜(-2)的高灵敏度,182 nM的低检测限,从6.0×10〜(-7)到8.0×10〜的宽线性范围(-4)M,高稳定性1个月。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号