CaO-SiO_2 glass-ceramic spheres were prepared by an electrospray method using hydrolyzed silicon alkoxide containing calcium nitrate. Crystalline calcium silicates, such as Ca_2SiOand β-CaSiO formed around the surface of the spheres after heat treatment. The dissolution of the crystal phase of the spheres caused the release of Ca~(2+) and Si~(4+) ions during the initial stage of soaking in Tris-buffer solution, leading to the formation of nanosized pores at the sphere surface. The incorporation of Ca~(2+) ions into the glassy phase of the spheres suppressed the rapid pH increase during the initial stage of soaking in Tris-buffer solution.
机译:通过使用含有硝酸钙的水解的硅醇盐的电喷雾法制备CaO-SiO_2玻璃陶瓷球。热处理后,在球体表面形成了结晶硅酸钙,例如Ca_2SiO和β-CaSiO。球晶相的溶解导致在Tris缓冲溶液中浸泡的初始阶段释放Ca〜(2+)和Si〜(4+)离子,从而导致在球体表面形成纳米孔。 。将Ca〜(2+)离子掺入球状玻璃态抑制了在Tris缓冲溶液中浸泡的初始阶段pH的快速增加。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号