A systematic review of the survival and complication rates of all-ceramic and metal-ceramic reconstructions after an observation period of at least 3 years. Part I: Single crowns.

机译:观察期至少三年后,对所有全瓷和金属陶瓷重建物的存活率和并发症发生率进行系统评价。第一部分:单冠。

获取原文
获取原文并翻译 | 示例
           

摘要

OBJECTIVES: The objective of this systematic review was to assess the 5-year survival rates of all-ceramic single crowns and to compare it with the survival rates of metal-ceramic crowns and to describe the incidence of biological and technical complications. METHODS: An electronic Medline and Dental Global Publication Research System search complemented by manual searching was conducted to identify prospective and retrospective cohort studies on all-ceramic and metal-ceramic crowns with a mean follow-up time of at least 3 years. Patients had to have been examined clinically at the follow-up visit. Assessment of the identified studies and data abstraction was performed independently by two reviewers. Annual failure rates were analyzed using standard and random-effects Poisson regression models to obtain summary estimates of survival proportions. RESULTS: The search provided 3473 titles and 177 abstracts. Full-text analysis was performed for 86 articles, resulting in 34 studies that met the inclusion criteria. In meta-analysis, the 5-year survival of all-ceramic crowns was estimated at 93.3% (95% confidence interval (CI): 91.1%-95%) and 95.6% (95% CI: 92.4%-97.5%) for metal-ceramic crowns. All-ceramic crowns were also analyzed according to the material utilized. Densely sintered alumina (Procera technique) crowns showed the highest 5-year survival rate of 96.4%, followed by reinforced glass-ceramic crowns (Empress technique) and InCeram-crowns with survival rates of 95.4% and 94.5%, respectively. A significantly lower survival rate of 87.5% was calculated for glass-ceramic crowns after 5 years. All-ceramic crowns were also grouped and analyzed regarding the position in the mouth. All four types of all-ceramic crowns showed lower survival rates when seated on posterior teeth. Moreover, for glass-ceramic crowns (84.4%) and InCeram-crowns (90.4%), this difference reached statistical significance (P = 0.009, P = 0.028). CONCLUSION: Based on the present systematic review, all-ceramic crowns, when used for anterior teeth, showed survival rates at 5 years comparable to those seen for metal-ceramic crowns. When used for posterior teeth, the survival rates at 5 years of densely sintered alumina crowns (94.9%) and reinforced glass-ceramic crowns (93.7%) were similar to those obtained for metal-ceramic crowns. Furthermore, lower survival rates of 90.4% and 84.4% can be expected for InCeram crowns and glass-ceramic crowns when utilized for premolars and molars.
机译:目的:本系统评价的目的是评估全瓷单冠的5年生存率,并将其与金属陶瓷冠的生存率进行比较,并描述生物学和技术并发症的发生率。方法:进行了电子Medline和牙科全球出版物研究系统搜索,并辅以人工搜索,以鉴定对全瓷和金属陶瓷冠的前瞻性和回顾性队列研究,平均随访时间至少为3年。必须在随访期间对患者进行临床检查。由两名审阅者独立进行鉴定研究和数据抽象的评估。使用标准和随机效应Poisson回归模型分析年度失败率,以获得生存比例的汇总估算。结果:搜索提供了3473个标题和177个摘要。对86篇文章进行了全文分析,得出34项符合纳入标准的研究。在荟萃分析中,全瓷冠的5年生存率估计为93.3%(95%置信区间(CI):91.1%-95%)和95.6%(95%CI:92.4%-97.5%)。金属陶瓷冠。还根据使用的材料对全瓷冠进行了分析。密集烧结的氧化铝冠(Procera技术)显示了最高的5年生存率,为96.4%,其次是增强玻璃陶瓷冠(Empress技术)和InCeram冠,其生存率分别为95.4%和94.5%。 5年后,玻璃陶瓷牙冠的存活率明显降低,为87.5%。还对全瓷冠进行了分组,并分析了它们在口腔中的位置。当坐在后牙上时,所有四种类型的全瓷冠都显示出较低的存活率。此外,对于玻璃陶瓷牙冠(84.4%)和InCeram牙冠(90.4%),这一差异达到统计学显着性(P = 0.009,P = 0.028)。结论:根据目前的系统评价,全瓷冠在用于前牙时的5年生存率与金属瓷冠相当。当用于后牙时,致密烧结的氧化铝冠(94.9%)和强化玻璃陶瓷冠(93.7%)在5年的存活率与金属陶瓷冠相似。此外,当将InCeram牙冠和玻璃陶瓷牙冠用于前磨牙和磨牙时,预期存活率会降低,分别为90.4%和84.4%。

著录项

相似文献

  • 外文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号