OBJECTIVES: A comparison of synthetic hydroxyapatite/silica oxide, xenogenic hydroxyapatite-based bone substitute materials with empty control sites in terms of bone regeneration enhancement in a rabbit calvarial four non-critical-sized defect model. METHODS: In each of six rabbits, four bicortical calvarial bone defects were generated. The following four treatment modalities were randomly allocated: (1) empty control site, (2) synthetic hydroxyapatite/silica oxide-based (HA/SiO) test granules, (3) xenogenic hydroxyapatite -based granules, (4) synthetic hydroxyapatite/silica oxide -based (HA/SiO) test two granules. The results of the latter granules have not been reported due to their size being three times bigger than the other two granule types. After 4 weeks, the animals were sacrificed and un-decalcified sections were obtained for histological analyses. For statistical analysis, the Kruskal-Wallis test was applied (P<0.05). RESULTS: Histomorphometric analysis showed an average area fraction of newly formed bone of 12.32+/-10.36% for the empty control, 17.47+/-6.42% for the xenogenic hydroxyapatite -based granules group, and 21.2+/-5.32% for the group treated with synthetic hydroxyapatite/silica oxide -based granules. Based on the middle section, newly formed bone bridged the defect to 38.33+/-37.55% in the empty control group, 54.33+/-22.12% in the xenogenic hydroxyapatite -based granules group, and to 79+/-13.31% in the synthetic hydroxyapatite/silica oxide -based granules group. The bone-to-bone substitute contact was 46.38+/-18.98% for the xenogenic and 59.86+/-14.92% for the synthetic hydroxyapatite/silica oxide-based granules group. No significant difference in terms of bone formation and defect bridging could be detected between the two bone substitute materials or the empty defect. CONCLUSION: There is evidence that the synthetic hydroxyapatite/silica oxide granules provide comparable results with a standard xenogenic bovine mineral in terms of bone formation and defect bridging in non-critical size defects.
机译:目的:在兔颅盖四头非关键性缺损模型中,比较合成的羟基磷灰石/氧化硅,异种羟基磷灰石基骨替代材料与空白对照位点的骨再生。方法:在每只六只兔中,产生了四只双皮质颅骨缺损。随机分配以下四种治疗方式:(1)空对照位点;(2)合成羟基磷灰石/氧化硅基(HA / SiO)测试颗粒;(3)异种羟基磷灰石基的颗粒;(4)合成羟基磷灰石/二氧化硅氧化物基(HA / SiO)测试两个颗粒。尚未报道后一种颗粒的结果,因为它们的大小是其他两种颗粒类型的三倍。 4周后,处死动物并获得未脱钙的切片用于组织学分析。为了进行统计分析,应用了Kruskal-Wallis检验(P <0.05)。结果:组织形态计量学分析显示,空对照组的新形成骨的平均面积分数为12.32 +/- 10.36%,异种羟基磷灰石基颗粒组的平均面积分数为17.47 +/- 6.42%,该组的平均面积分数为21.2 +/- 5.32%用合成的羟基磷灰石/氧化硅基颗粒处理。在中间部分的基础上,新形成的骨将缺损对照组中的缺损桥接至38.33 +/- 37.55%,异种羟基磷灰石基颗粒组中的桥接缺损为54.33 +/- 22.12%,而在异体羟基磷灰石基颗粒组中则桥接至79 +/- 13.31%。合成的基于羟基磷灰石/二氧化硅的颗粒组。异种的骨-骨替代接触为46.38 +/- 18.98%,而合成的羟基磷灰石/氧化硅基颗粒组为59.86 +/- 14.92%。在两种骨替代材料或空缺之间,在骨形成和缺损桥接方面没有发现显着差异。结论:有证据表明,合成的羟基磷灰石/氧化硅颗粒在非关键尺寸缺陷的骨形成和缺陷桥接方面可提供与标准异种牛矿物相当的结果。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号