Clinopyroxenes of the join CaMgSi2O6(diopside)-NaAlSi2O6 (jadeite) were synthesized in the temperature range 800-1900 degrees C and under varying pressure, 10-55 kbar. The stability regions of various compositions of diopside-jadeite have been established experimentally using different compositions of glass materials: stoichiometric composition NaAlSi2O6, 0.1CaMgSi(2)O(6)-0.9NaAlSi(2)O(6), 0.2CaMgSi(2)O(6)0.8NaAlSi(2)O(6), 0.3CaMgSi(2)O(6)-0.7NaAlSi(2)O(6), and 0.4CaMgSi(2)O(6)-0.6NaAlSi(2)O(6). Unit cell parameters of synthetic clinopyroxenes with the above compositions were determined. The physical properties, such as hardness, toughness, density, and refractive index, etc., were also measured. The results show that synthetic clinopyroxenes have the same properties as the natural one. The gem quality of diopside-jadeite clinopyroxenes was achieved by synthesised on the basis of the above experiments. Various colouring agents, such as Cr2O3, Co2O3, NiO2, Fe2O3, TiO2, MnO, CuO, and their combinations, FeO-Cr2O3, etc., were added to obtain the different colours of gem. In addition, small amounts of the rare-earth oxides, such as CeO2, Nd2O3, Sm2O3, Dy2O3, Eu2O3, Er2O3, Pr6O11, Lu2O3 and CuO-Eu2O3, Co2O3Nd2O3, etc., were also added to produce fluorescent clinopyroxenes for jewellery. [References: 23]
机译:CaMgSi2O6(透辉石)-NaAlSi2O6(硬玉)的亚环己基亚砜在800-1900摄氏度的温度范围和10-55 kbar的变压下合成。已使用不同的玻璃材料组成通过实验确定了透辉石-硬玉的各种组成的稳定区域:化学计量组成NaAlSi2O6、0.1CaMgSi(2)O(6)-0.9NaAlSi(2)O(6),0.2CaMgSi(2) O(6)0.8NaAlSi(2)O(6),0.3CaMgSi(2)O(6)-0.7NaAlSi(2)O(6)和0.4CaMgSi(2)O(6)-0.6NaAlSi(2) O(6)。测定具有上述组成的合成环吡咯的晶胞参数。还测量了诸如硬度,韧性,密度和折射率等的物理性质。结果表明,合成的clinopyroxenes具有与天然的相同的性质。在上述实验的基础上,通过合成获得了透辉石-翡翠亚铁辉石的宝石品质。添加各种着色剂,例如Cr2O3,Co2O3,NiO2,Fe2O3,TiO2,MnO,CuO及其组合,FeO-Cr2O3等,以获得宝石的不同颜色。此外,还添加了少量稀土氧化物,例如CeO2,Nd2O3,Sm2O3,Dy2O3,Eu2O3,Er2O3,Pr6O11,Lu2O3和CuO-Eu2O3,Co2O3Nd2O3等,以生产用于珠宝的荧光金烛石。 [参考:23]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号