DIELECTRIC AND ELECTRICAL PROPERTIES OF ORDINARY PORTLAND CEMENT AND SLAG CEMENT IN THE EARLY HYDRATION PERIOD

机译:水化初期普通硅酸盐水泥和矿渣水泥的介电性能

获取原文
获取原文并翻译 | 示例
           

摘要

The dielectric constant and electrical conductivity of ordinary Portland cement (OPC) with water-cement ratios (w/c) of 0.30, 0.35 and 0.40 were measured for the first 30 h hydration, using a microwave technique in the frequency range 8.2-12.4 GHz. It was found that both the dielectric constant and electrical conductivity of the cement paste are sensitive to the water-cement ratio, the higher the w/c value, the greater the dielectric constant and electrical conductivity, and the longer the hydration time. We also found that the higher the frequency the greater the electrical conductivity but the smaller the dielectric constant. The dielectric constant and electrical conductivity of high- and low-slag cement with water-solid ratio (w/s) of 0.40 were measured in the first 30 h after mixing. The changes in dielectric constant and electrical conductivity of low-slag cement with time are similar to that of OPC, but the high-slag cement shows very different dielectric and electrical properties compared with OPC and low-slag cement. The relationship between the dielectric and electrical properties of cement paste and cement hydration was also discussed. [References: 36]
机译:使用微波技术在8.2-12.4 GHz频率范围内水合的前30小时测量了水灰比(w / c)为0.30、0.35和0.40的普通硅酸盐水泥(OPC)的介电常数和电导率。已发现水泥浆的介电常数和电导率均对水灰比敏感,w / c值越高,介电常数和电导率越大,水合时间越长。我们还发现,频率越高,电导率越大,但介电常数越小。在混合后的最初30小时内,测量水固比(w / s)为0.40的高矿渣水泥和低矿渣水泥的介电常数和电导率。低矿渣水泥的介电常数和电导率随时间的变化与OPC相似,但与OPC和低矿渣水泥相比,高矿渣水泥的介电性能和电性能差异很大。还讨论了水泥浆的介电和电性能与水泥水化之间的关系。 [参考:36]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号