Objectives: To determine the degree of conversion (DC) and Knoop microhardness (KHN) of resin-based composites (RBCs) containing trimethylbenzoyl-diphenylphosphine oxide (TPO) cured by polywave or monowave LED light-curing units (LCUs). Methods: Three groups (each n = 5) of Tetric EvoCeram (Ivoclar Vivadent), Vit-l-escence (Ultradent) and Herculite XRV Ultra (Kerr) were prepared in Teflon moulds (5 mm in diameter and 2 mm thick) and cured with polywave Bluephase ? G2 (Ivoclar Vivadent), polywave Valo (Ultradent) or monowave Bluephase ? (Ivoclar Vivadent; control) resulting in 9 groups. DC and KHN were determined using micro-Raman spectroscopy and Knoop microhardness, respectively. High-performance liquid chromatography and nuclear magnetic resonance spectroscopy were used to confirm the presence or absence of TPO in the three uncured materials. Data were statistically analysed using two-way and one-way ANOVA and DC and KHN were correlated using Pearson's correlation (α = 0.05). Results: TPO was confirmed in Tetric EvoCeram and Vit-l-escence but not in Herculite XRV Ultra. All three LCUs produced comparable KHN for Tetric EvoCeram and Herculite XRV Ultra (p 0.05). Both polywave LCUs resulted in significantly higher KHN for Vit-l-escence and higher DC in Tetric EvoCeram and Vit-l-escence than the monowave Bluephase ? (p 0.05). Conversely, Bluephase ? showed higher DC than the two polywave LCUs in Herculite XRV Ultra (p 0.05). Pearson's correlation coefficient was r = 0.818. Conclusions: Polywave LED LCUs improved monomer to polymer conversion and KHN in the two TPO-containing RBCs, but not in Herculite XRV Ultra. DC and KHN were linearly correlated in all three RBCs. Vit-l-escence showed the highest DC and KHN of the three materials tested. Clinical significance: The use of polywave LEDs significantly improves both the DC and KHN of materials which contain TPO. This should be taken into account when curing bleached shades of RBCs even if the manufacturers do not indicate the presence of TPO in their materials.
机译:目的:确定通过多波或单波LED光固化单元(LCU)固化的包含三甲基苯甲酰基-二苯基氧化膦(TPO)的树脂基复合材料(RBC)的转化度(DC)和努氏显微硬度(KHN)。方法:在特氟隆模具(直径5毫米,厚度2毫米)中制备三组(每组n = 5)Tetric EvoCeram(Ivoclar Vivadent),Vit-l-escence(Ultradent)和Herculite XRV Ultra(Kerr)并固化与多波Bluephase吗? G2(Ivoclar Vivadent),多波Valo(Ultradent)或单波Bluephase? (Ivoclar Vivadent;对照)分成9组。 DC和KHN分别使用显微拉曼光谱法和努氏显微硬度法测定。高效液相色谱法和核磁共振波谱法用于确认三种未固化材料中是否存在TPO。使用双向和单向方差分析对数据进行统计分析,并使用皮尔逊相关系数(α= 0.05)将DC和KHN进行关联。结果:在Tetric EvoCeram和Vit-1发光中证实了TPO,但在Herculite XRV Ultra中未证实。对于Tetric EvoCeram和Herculite XRV Ultra,这三个LCU均产生了可比的KHN(p> 0.05)。两种多波LCU均导致Vit-1发光的KHN显着升高,而Tetric EvoCeram和Vit-1发光的DC显着高于单波Bluephase? (p <0.05)。相反,Bluephase?在Herculite XRV Ultra中显示出比两个多波LCU更高的DC(p <0.05)。皮尔逊相关系数为r = 0.818。结论:Polywave LED LCU在两个含TPO的RBC中改善了单体到聚合物的转化和KHN,但在Herculite XRV Ultra中却没有。 DC和KHN在所有三个RBC中均呈线性相关。维生素L发光显示了三种测试材料中最高的DC和KHN。临床意义:多波LED的使用显着改善了含有TPO的材料的DC和KHN。即使制造商未指出其材料中存在TPO,在固化RBC的漂白色调时也应考虑到这一点。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号