OBJECTIVE: This study examined temporary restorative resins that use non-phthalate ester plasticizers. METHODS: Three non-phthalate plasticizers were tested: tri-ethyl citrate (TEC), tri-butyl citrate (TBC), and di-butyl sebacate (DBS). The experimental resins were compared with resins that use a phthalate ester plasticizer (di-butyl phthalate, DBP) and commercial products (Dura Seal, Plast Seal, and Fit Seal). For the experimental resins, the ratio of plasticizer to PMMA/MMA resin was varied from 30 to 60% (wt). The mechanical properties of the experimental resins were evaluated using a modified diametral compressive strength and the resistance to explorer insertion. RESULTS: The strengths of the experimental resins with plasticizer concentrations ranging from 40 to 50% (TEC, TBC, and DBP) or from 30 to 40% (DBS), by weight, were equivalent to the strengths of commercial temporary restorative resins. A similar tendency was seen for the resistance to explorer insertion. CONCLUSIONS: The results suggestthat new temporary restorative resins can be prepared by choosing the appropriate proportions of resin monomer and non-phthalate ester plasticizer.
机译:目的:本研究检查了使用非邻苯二甲酸酯增塑剂的临时修复树脂。方法:测试了三种非邻苯二甲酸酯增塑剂:柠檬酸三乙酯(TEC),柠檬酸三丁酯(TBC)和癸二酸二丁酯(DBS)。将实验树脂与使用邻苯二甲酸酯增塑剂(邻苯二甲酸二丁酯,DBP)和商业产品(Dura Seal,Plast Seal和Fit Seal)的树脂进行了比较。对于实验树脂,增塑剂与PMMA / MMA树脂的比例在30%(重量)至60%(重量)之间变化。使用改良的直径抗压强度和抗探索者插入的能力评估了实验树脂的机械性能。结果:增塑剂浓度范围为40%至50%(TEC,TBC和DBP)或30%至40%(DBS)的实验树脂的强度(按重量计)与商用临时修复树脂的强度相当。对于浏览器插入的阻力也看到了类似的趋势。结论:结果表明,可以通过选择适当比例的树脂单体和非邻苯二甲酸酯增塑剂来制备新型临时修复树脂。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号