首页> 外文期刊>Journal of biomedical materials research. Part B, Applied biomaterials. >Self-Reinforced Polylactide/Polyglycolide 80/20 Screws Take More Than 1(1/2) Years to Resorb in Rabbit Cranial Bone;;Self-Reinforced Polylactide/Polyglycolide 80/20 Screws Take More Than 1(1/2) Years to Resorb in Rabbit Cranial Bone
【24h】

Self-Reinforced Polylactide/Polyglycolide 80/20 Screws Take More Than 1(1/2) Years to Resorb in Rabbit Cranial Bone;;Self-Reinforced Polylactide/Polyglycolide 80/20 Screws Take More Than 1(1/2) Years to Resorb in Rabbit Cranial Bone

机译:自增强聚丙交酯/聚乙交酯80/20螺钉需要超过1(1/2)年才能吸收兔颅骨;;自增强聚丙交酯/聚乙交酯80/20螺钉要吸收超过1(1/2)年在兔颅骨中

获取原文
获取原文并翻译 | 示例
       

摘要

The aim of this study was to assess tissue reactions to bioabsorbable self-reinforced polylactide/polyglycolide (SR-PLGA) 80/20 miniscrews in rabbit cranial bone. One PLGA screw was implanted on one side and one titanium screw on the other side of the sagittal suture (n = 21). Three animals were sacrificed after 2, 4, 8, 16, 24, 54, and 72 weeks. In histological examination the numbers of macrophages, giant cells, active osteoblasts, and fibrous tissue layers were assessed and degradation of the bioabsorbable screws was evaluated. After 2 weeks, macrophages were seen near the heads of both screws. After 4 and 8 weeks, the bioabsorbable screws were surrounded by fibrous tissue. Osteoblastic activity and groups of several giant cells were seen. After 24 weeks, a significant change in the morphology of the PLGA screws had occurred. Osteoblastic activity and the amount of giant cells had decreased. After 1 year, some PLGA biomaterial was still present. PLGA screws had been replaced by adipose tissue, fibrous tissue, and "foamy macrophages" that had PLGA particles inside them. After 1(1/2) years, the amount of biomaterial remaining had decreased remarkably. The particles of biomaterial were inside foamy macrophages. SR-PLGA 80/20 screws are biocompatible and have no clinically manifested complications when used in the cranial bone of rabbits. No contraindications as regards their clinical use in craniofacial surgery was found when these screws were studied in the cranial bones of rabbits.
机译:本研究的目的是评估兔颅骨中对生物可吸收的自增强聚乳酸/聚乙交酯(SR-PLGA)80/20微螺钉的组织反应。在矢状缝合线的一侧植入一个PLGA螺钉,在另一侧植入一个钛螺钉(n = 21)。在2、4、8、16、24、54和72周后处死三只动物。在组织学检查中,评估巨噬细胞,巨细胞,活性成骨细胞和纤维组织层的数量,并评估生物可吸收螺钉的降解。 2周后,在两个螺钉的头部附近看到巨噬细胞。 4和8周后,生物可吸收螺钉被纤维组织包围。观察到成骨细胞活性和几个巨型细胞的组。 24周后,PLGA螺钉的形态发生了显着变化。成骨细胞活性和巨细胞数量减少。一年后,仍然存在一些PLGA生物材料。 PLGA螺钉已被脂肪组织,纤维组织和内部含有PLGA颗粒的“泡沫巨噬细胞”所取代。 1(1/2)年后,生物材料的残留量显着减少。生物材料的颗粒位于泡沫巨噬细胞内部。 SR-PLGA 80/20螺钉具有生物相容性,在兔子的颅骨中使用时没有临床表现的并发症。当在兔子的颅骨中研究这些螺钉时,没有发现关于它们在颅面部手术中的临床使用的禁忌症。