The effects of two nonreactive conventional-type resins, a bisphenol-Abased phenoxy resin PAPHEN-301 and aromatic-based PETROLEUM RESIN, on the mechanical, thermal, and physical properties of methacrylated urethane resin-based W-curable formulations were studied. A methacrylated urethane prepolymer was synthesized from isocyanatoethyl methacrylate (IEM) and polytetrahydrofurandiol (PTHF) via a one-step reaction. An increase in PAPHEN-301 content caused an increase both in tensile strength and elongation values of UV-cured polymeric films. On the other hand, an increase in PETROLEUM RESIN content caused a decrease both in tensile strength and elongation values of the polymeric films. However, thermooxidative properties were not affected by the introduction of either resin. It was also found that the water-absorption capacities of the UV-cured methacrylated urethane films depended on the type and amount of the nonreactive resins. (C) 1998 John Wiley & Sons, Inc. J Appl Polym Sci 69: 1831-1845, 1998. [References: 13]
机译:研究了两种非反应性常规类型树脂,即双酚A基苯氧基树脂PAPHEN-301和芳族基石油树脂对甲基丙烯酸聚氨酯树脂基W固化配方的机械,热和物理性能的影响。通过一步反应,由甲基丙烯酸异氰酸根合乙酯(IEM)和聚四氢呋喃二醇(PTHF)合成甲基丙烯酸酯化的聚氨酯预聚物。 PAPHEN-301含量的增加导致UV固化聚合物薄膜的拉伸强度和伸长率值均增加。另一方面,石油树脂含量的增加引起聚合物膜的拉伸强度和伸长率值的降低。但是,热氧化性能不受任何一种树脂的引入的影响。还发现,UV固化的甲基丙烯酸酯化的聚氨酯膜的吸水能力取决于非反应性树脂的类型和量。 (C)1998 John Wiley&Sons,Inc. J Appl Polym Sci 69:1831-1845,1998。[参考:13]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号