Graft copolymers containing poly(ethylene oxide) side chains attached to a polyethylene backbone were prepared by coupling of poly(ethylene-co-acrylic acid) (PEAA) and poly(ethylene oxide) monomethyl ethers (MPEO) by esterification in o-xylene at 140 degrees C. The MPEO side chains had molecular weights of 750 to 5000. The chemical composition of the graft copolymers was analyzed by NMR and FT-IR spectroscopy. The weight fraction of the MPEO grafts in the graft copolymers was found to be around 0.4. The graft copolymers exhibited a phase-separated morphology with the backbones and the MPEO grafts forming separate crystalline phases. The MPEO phase had a melting temperature 8-25 degrees C lower than the corresponding MPEO homopolymers, as determined by DSC. The melting point of the crystalline phase formed by the PEAA main chains was close to that of the pure PEAA. Crystallinity was also confirmed by x-ray diffraction. (C) 1996 John Wiley & Sons, Inc. [References: 20]
机译:通过在邻二甲苯中进行酯化反应,将聚(乙烯-共丙烯酸)(PEAA)和聚(环氧乙烷)单甲醚(MPEO)偶联,制得含有连接至聚乙烯主链的聚(环氧乙烷)侧链的接枝共聚物。 140℃。MPEO侧链的分子量为750至5000。通过NMR和FT-IR光谱分析接枝共聚物的化学组成。发现接枝共聚物中MPEO接枝的重量分数为约0.4。接枝共聚物表现出相分离的形态,主链和MPEO接枝形成单独的结晶相。通过DSC测定,MPEO相的熔融温度比相应的MPEO均聚物低8-25℃。 PEAA主链形成的结晶相的熔点接近纯PEAA的熔点。结晶度也通过X射线衍射确认。 (C)1996 John Wiley&Sons,Inc. [参考:20]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号