The influence of a beta-diketone on the already observed anomalous behavior of preheated metal stearates as stabilizers for PVC has been evaluated. During normal stabilization procedure, the addition of diketones reduce the stabilization times, but the pretreatment of the mixture of metal soaps or of the individual zinc soap (then added to the calcium soap) delayed such times, recovering to some extent the reduction induced by the costabilizer. The calcium soap preheated (added along with zinc stearate to PVC), on the other hand, reduced the induction times further. These findings obtained by measurement of induction times by means of loss of weight (TGA) and HCl evolution, have been supported by FTIR and visible reflectance studies. While using preheated ZnSt(2), a second rate of dehydrochlorination was observed in the HCl evolution traces, suggesting a separate consumption of the compounds during the stabilization mechanism. In general, it can be said that preheated primary stabilizers and costabilizers have no significant interactions between them. The final result is just the addition of their separate effects. (C) 1998 John Wiley & Sons, Inc. [References: 19]
机译:已经评估了β-二酮对已经观察到的预热金属硬脂酸盐作为PVC稳定剂的异常行为的影响。在正常的稳定程序中,添加二酮会减少稳定时间,但是金属皂混合物或单个锌皂(然后添加到钙皂中)的预处理会延迟这种时间,在一定程度上可以恢复由金属皂引起的还原。稳定剂。另一方面,预热的钙皂(与硬脂酸锌一起添加到PVC中)进一步缩短了诱导时间。通过FTIR和可见反射研究支持了通过失重(TGA)和HCl析出的诱导时间测量获得的这些发现。当使用预热的ZnSt(2)时,在HCl析出痕迹中观察到第二个脱氯化氢速率,表明在稳定机理期间化合物的单独消耗。通常,可以说预热的主稳定剂和共稳定剂之间没有明显的相互作用。最终结果只是添加了它们各自的效果。 (C)1998 John Wiley&Sons,Inc. [参考:19]

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号