A description is given of a new form of droplet erosion of titanium condenser tubese. At the sites of maximum impact by wet steam, the tube wall thickness is reduced to zero, and the tubes crack open under pressure of the cooling water .The crack is unbranched and porgresses in a stepwise fashion. Along one side of the crack a series of small, circular metallic protrusions develops. Microscopic examination reveals the absence of any corrosion products on the surface. Similarly, no feather-like structure indicative of hydride formation is noted. It is assumed that impact with wet steam produces high-pressure transients and initiates high flow away from the points of impact. Counter-measures against droplet erosion are briefly reviewed and involve the reduction of steam velocity and/or degree of wetness. Plugging of the defected tubes is another practical means, and the use of protective sleeves might also be considered. Rutubing with a more erosion-resitant material might present an ultimate, more feasible solution.
机译:给出了钛冷凝器管的液滴侵蚀的一种新形式的描述。在湿蒸汽最大冲击的位置,管壁厚度减小到零,并且在冷却水的压力下,管子开裂。裂缝是无分支的,并且呈阶梯状扩展。沿着裂纹的一侧会出现一系列小的圆形金属突起。显微镜检查表明表面上没有任何腐蚀产物。类似地,没有注意到指示氢化物形成的羽毛状结构。假定湿蒸汽的撞击会产生高压瞬变,并引发远离撞击点的高流量。简要回顾了防滴蚀的对策,涉及降低蒸汽速度和/或降低湿度的方法。堵塞有缺陷的管子是另一种实用的方法,也可以考虑使用保护套。用更耐腐蚀的材料制成的风琴可以提供一种最终的,更可行的解决方案。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号