Nonwoven viscose fabric was treated with chitosan/polyvinyl alcohol (PVA) using pad-dry method, using different concentrations of chitosan and PVA. Increasing the amount of PVA leads to increasing of air permeability. Water permeability increased by increasing the amount of PVA to 2 ml (10% solution) then decreased by any increase of the quantity of PVA solution. Roughness increased with increasing the amount of 10% PVA solution. It is shown that roughness, water and air permeability increased with increasing the chitosan concentration. Antibacterial properties was increased with increasing PVA/or chitosan concentration. The chitosan/PVA treated nonwoven viscose fabric was immersed in a solution of Ag nanoparticles. The chitosan/PVA/Ag nanoparticles treated nonwoven fabrics were used as wound dressings on French white Bouscat rabbits, with age ranged from 1 to 2 years. A complete healing was achieved using wound dressing consists of nonwoven viscose fabric treated with chitosan/PVA/Ag nanoparticles after 21 days. The histopathological examination confirmed the complete re-epithelialization and averagely thick epidermis formation.
机译:非织造粘胶纤维织物是通过垫干法用壳聚糖/聚乙烯醇(PVA)处理的,其中使用了不同浓度的壳聚糖和PVA。 PVA的量增加导致透气性增加。通过将PVA的量增加到2 ml(10%溶液)来增加透水性,然后通过增加PVA的溶液量来降低透水性。粗糙度随着10%PVA溶液量的增加而增加。结果表明,随着壳聚糖浓度的增加,粗糙度,水和空气透过率增加。抗菌性能随PVA /或壳聚糖浓度的增加而增加。将壳聚糖/ PVA处理的非织造粘胶织物浸入Ag纳米颗粒溶液中。壳聚糖/ PVA / Ag纳米粒子处理的非织造织物被用作法国白色Bouscat兔的伤口敷料,年龄在1-2岁之间。 21天后,使用由壳聚糖/ PVA / Ag纳米粒子处理的无纺粘胶织物制成的伤口敷料即可实现完全愈合。组织病理学检查证实完全上皮再形成和平均厚的表皮形成。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号