The present paper reports the graft copolymerization of N-vinylformamide onto sodium carboxymethylcellulose by free radical polymerization using potassium peroxymonosulphate/thiourea redox system in an inert atmosphere. The reaction conditions for maximum grafting have been optimized by varying the reaction variables, including the concentration of N-vinylformamide (12.0 x 10~(-2)-28.0 x 10~(-2) mol dm~(-3)), potassium peroxymonosulphate (4.0 x 10~(-3)-12.0 x 10~(-3) mol dm~(-3)), thiourea (1.2 x 10~(-3)-4.4 x 10~(-3) mol dm~(-3)), sulphuric acid (2.0 x 10~(-3)-10.0 x 10~(-3) mol dm~(-3)), sodium carboxymethylcellulose (0.2-1.8 g dm~(-3)) along with time duration (60-180 min) and temperature (25-45° C). Water swelling capacity, metal ion sorption and flocculation studies of synthesized graft copolymer have been performed with respect to the parent polymer. The graft copolymer has been characterized by FTIR spectroscopy and thermogravimetric analysis.
机译:本论文报道了在惰性气氛下使用过氧单硫酸钾/硫脲氧化还原体系通过自由基聚合将N-乙烯基甲酰胺接枝共聚合到羧甲基纤维素钠上。通过改变反应变量,包括N-乙烯基甲酰胺的浓度(12.0 x 10〜(-2)-28.0 x 10〜(-2)mol dm〜(-3)),钾离子,优化了最大接枝反应条件。过氧单硫酸盐(4.0 x 10〜(-3)-12.0 x 10〜(-3)mol dm〜(-3)),硫脲(1.2 x 10〜(-3)-4.4 x 10〜(-3)mol dm〜 (-3)),硫酸(2.0 x 10〜(-3)-10.0 x 10〜(-3)mol dm〜(-3)),羧甲基纤维素钠(0.2-1.8 g dm〜(-3))持续时间(60-180分钟)和温度(25-45°C)。对于母体聚合物已经进行了合成接枝共聚物的水溶胀能力,金属离子吸附和絮凝研究。接枝共聚物已经通过FTIR光谱和热重分析进行了表征。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号