The preparation of thin films of chitosan-silane hybrid materials by combining sol-gel processing and spin coating is reported. A variety of silanes can be used as starting materials for the preparation of such thin films, namely tetraethoxysilane, tri-tert-butoxysilanol, trimethylethoxysilane, p-trifluoromethyltetra-fluorophenyltriethoxysilane,trivinylmethoxysilane,(methoxymethyl)trimethyl-silane, and hexamethoxydisilane. These silanes are subjected to a sol-gel process before they are added to acidic chitosan solutions. The chitosan-.silane ratio is kept constant at 6:1 (w/w) and dilutions with ethanol are prepared and spin coated. Depending on the degree of dilution, film thickness can be controlled in a range between 5 and 70 nm. For the determination of additional surface properties, static water contact angle measurements and atomic force microscopy have been employed.
机译:报道了通过结合溶胶-凝胶法和旋涂法制备壳聚糖-硅烷杂化材料薄膜。各种硅烷可以用作制备这种薄膜的原料,即四乙氧基硅烷,三叔丁氧基硅烷醇,三甲基乙氧基硅烷,对三氟甲基四氟苯基三乙氧基硅烷,三乙烯基甲氧基硅烷,(甲氧基甲基)三甲基硅烷和六甲氧基二硅烷。在将这些硅烷添加到酸性壳聚糖溶液中之前,先对其进行溶胶-凝胶工艺。壳聚糖与硅烷的比率保持恒定在6:1(w / w),并用乙醇稀释并旋涂。取决于稀释度,可以将膜厚度控制在5至70nm之间的范围内。为了确定其他表面性能,已采用静态水接触角测量和原子力显微镜。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号