首页> 外文期刊>Topics in Catalysis >Preservation of the Activity of Supported Gold Catalysts for CO Oxidation
【24h】

Preservation of the Activity of Supported Gold Catalysts for CO Oxidation

机译:保留负载型金催化剂用于CO氧化的活性

获取原文
获取原文并翻译 | 示例
           

摘要

Procedures leading to the preservation of activity of supported gold catalysts for CO oxidation are reviewed. The inclusion of iron as Fe(OH)_3 in preparing catalysts using tin oxide, ceria and zirconia as supports gives better activity and much improved stability with time-on-stream. In the case of Au/Fe-SnO2 (0.5-0.9% Au), the effect is maximal with ~4% Fe. The stability of catalysts based on ceria as support is also much better when small amounts of either iron or lanthanum during preparation of the support by thermal decomposition of nitrates. Au/SnO2 catalysts often suffer initial deactivation followed by an increase in activity with time-on-stream; a period of refrigeration (7d) induces an excellent stability at high conversion.
机译:本文综述了导致负载型金催化剂保持CO氧化活性的方法。在使用氧化锡,二氧化铈和氧化锆作为载体的制备催化剂中包含铁作为Fe(OH)_3可以提供更好的活性并大大提高其在运行时间上的稳定性。在Au / Fe-SnO2(0.5-0.9%Au)的情况下,Fe含量约为4%时效果最大。当通过硝酸盐的热分解制备载体时,当少量的铁或镧时,基于二氧化铈作为载体的催化剂的稳定性也要好得多。 Au / SnO2催化剂通常会遭受初始失活,随后随着生产时间的延长而活性增加;一段冷藏(7d)在高转化率下具有极好的稳定性。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号