Fly ash and bottom ash, the two main by-products of thermal power plant, have been used synergistically to develop geopolymer concrete. Fly ash has been used as active constituent for geopolymerization whereas bottom ash has been used as replacement of sand. Geopolymerization studies were carried out at ambient (27 degrees C) and elevated (55 degrees C) temperatures using isothermal conduction calorimetry. The reaction product was characterized using X-ray diffraction (XRD) and scanning electron microscopy (SEM). The geopolymer concrete prepared at 60 degrees C showed compressive strength in the range of 4-35 MPa. Strength development was studied as a function of alkali concentration and Si/Al ratio. It was observed that strength got improved significantly with higher alkali concentration and Si/Al ratio. Attempt has been made to correlate the structure with properties.
机译:粉煤灰和底灰是火力发电厂的两个主要副产品,已被协同使用来开发地聚合物。粉煤灰已被用作地聚合的活性成分,而底灰已被用作砂的替代品。使用等温传导量热法在环境温度(27摄氏度)和升高的温度(55摄氏度)下进行了地质聚合研究。使用X射线衍射(XRD)和扫描电子显微镜(SEM)表征反应产物。在60摄氏度下制备的地质聚合物混凝土的抗压强度为4-35 MPa。研究了强度发展与碱浓度和Si / Al比的关系。观察到强度随着碱浓度和Si / Al比的增加而显着提高。已经尝试将结构与特性相关联。

著录项

相似文献

  • 外文文献
  • 中文文献
  • 专利
获取原文

客服邮箱:kefu@zhangqiaokeyan.com

京公网安备:11010802029741号 ICP备案号:京ICP备15016152号-6 六维联合信息科技 (北京) 有限公司©版权所有
  • 客服微信

  • 服务号